DOI QR코드

DOI QR Code

지르코니아 코핑과 전장도재 간의 전단결합강도와 파절양상 비교

A comparative study of the shear bond strength and failure mode between zirconia copings and veneering ceramics

  • 김원영 (부산가톨릭대학교 보건과학대학 치기공학과, 치과기공기재학회) ;
  • 전병욱 (부산가톨릭대학교 보건과학대학 치기공학과, 치과기공기재학회) ;
  • 정인성 (부산가톨릭대학교 보건과학대학 치기공학과, 치과기공기재학회)
  • Kim, Won-Young (Dept. of Dental Laboratory Science, College of Health Science, Catholic University of Pusan) ;
  • Jeon, Byung-Wook (Dept. of Dental Laboratory Science, College of Health Science, Catholic University of Pusan) ;
  • Chung, In-Sung (Dept. of Dental Laboratory Science, College of Health Science, Catholic University of Pusan)
  • 투고 : 2015.10.30
  • 심사 : 2015.12.18
  • 발행 : 2015.12.30

초록

Purpose: The aim of this study was to investigate the shear bond strength between various commercial zirconia coping and veneering ceramic, and to observe the failure mode. Methods: For each zirconia block (iJAM Emerald, LUXEN Smile block, ICE Zirkon transluzent), 10 rectangular specimens were layered with Cercon ceram kiss, IPS e.max ceram, ICE Zirkon ceramic according to recommended by the manufacturer. The shear bond strength tests of the veneering porcelain to zirconia were carried out until fracture by a universal testing machine. After the shear bond tests, failure modes were characterized visually, under a stereomicroscope, such as adhesive, cohesive, or mixed. Data were analyzed with One-way ANOVA followed by Scheffe's tests. Results: The shear bond strength ($mean{\pm}SD$) of zirconia-veneer ceramic were JC group $13.9{\pm}3.6MPa$; JE group $17.7{\pm}2.4MPa$; JI group $15.1{\pm}2.5MPa$; LC group $9.5{\pm}1.5MPa$; LE group $16.2{\pm}2.3MPa$; LI group $12.6{\pm}0.8MPa$; ZC group $16.0{\pm}2.3MPa$; ZE group $18.5{\pm}3.4MPa$; and ZI group $15.3{\pm}3.2MPa$. The One-way ANOVA showed a significant difference between groups (p<0.05). The failure mode in most experimental groups was mixed failure, except for the LC group, which showed adhesive failure, and JE group, LE group and ZE group showed cohesive failure. Conclusion: For IPS e.max ceram, the shear bond strength value was highest for all kinds of zirconia blocks. For ICE Zirkon transluzent, the shear bond strength value was highest for all kinds of veneering ceramics. Most of experimental group interfaces revealed mixed failure mode.

키워드

참고문헌

  1. Aboushelib MN, De Jager N, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater, 21(10), 984-991, 2005. https://doi.org/10.1016/j.dental.2005.03.013
  2. Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Effect of zirconia type on its bond strength with different veneer ceramics. J Prosthodont, 17(5), 401-408, 2008. https://doi.org/10.1111/j.1532-849X.2008.00306.x
  3. Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering ceramics. Dent Mater, 22(9), 857-863, 2006. https://doi.org/10.1016/j.dental.2005.11.014
  4. Albakry M, Guazzato M, Swain MV. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials. J Dent, 31(3), 181-188, 2003. https://doi.org/10.1016/S0300-5712(03)00025-3
  5. Al-Dohan HM, Yaman P, Dennison JB, Razzoog ME, Lang BR. Shear strength of core-veneer interface in bi-layered ceramics. J Prosthet Dent, 91(4), 349-355, 2004. https://doi.org/10.1016/j.prosdent.2004.02.009
  6. Cardoso PE, Sadek FT, Goracci C, Ferrari M. Adhesion testing with the microtensile method: effects of dental substrate and adhesive system on bond strength measurements. J Adhes Dent, 4(4), 291-297, 2002.
  7. El Zohairy AA, De Gee AJ, Mohsen MM, Feilzer AJ. Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks. Dent Mater, 19(7), 575-583, 2003. https://doi.org/10.1016/S0109-5641(02)00107-0
  8. Fischer J, Stawarczyk B, Sailer I, Hammerle CHF. Shear bond strength between veneering ceramics and ceria-stabilized zirconia/ alumina. J Prosthet Dent, 103(5), 267-274, 2010. https://doi.org/10.1016/S0022-3913(10)60056-X
  9. Guess PC, Kulis A, Witkowski S, Wolkewitz M, Zhang Y, Strub JR. Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling. Dent Mater, 24(11), 1556-1567, 2008. https://doi.org/10.1016/j.dental.2008.03.028
  10. Hamid MA, Ariel JR, Brian DF, Harald H, Lloyd AM. Flexural and shear strength of $ZrO_2$ and a high-noble alloy bonded to their corresponding porcelains. J Prosthet Dent, 100(4), 274-284, 2008. https://doi.org/10.1016/S0022-3913(08)60206-1
  11. Jang SA, Kim YY, Park WH, Lee YS. Comparative study of fracture strength depending on the occlusal thickness of full zirconia crown. J Korean Acad Prosthodont, 51(3), 160-166, 2013. https://doi.org/10.4047/jkap.2013.51.3.160
  12. Juy A, Anglada M. Surface phase transformation during grinding of Y-TZP. J Am Ceram Soc, 90(8), 2618-2621, 2007. https://doi.org/10.1111/j.1551-2916.2007.01739.x
  13. Kim JM, Bae JM, Oh SH. The effect of thermocycling on the shear-bond strength of ceramic core-porcelain veneer. Kor J Dent Mater, 40(2), 87-94, 2013.
  14. Kim WY, Chung IS, Jeon BW. Comparison of mechanical properties of all ceramic crown on zirconia blocks. J Kor Aca Den Tec, 37(3), 107-113, 2015. https://doi.org/10.14347/kadt.2015.37.3.107
  15. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. Strength and reliability of surface treated Y-TZP dental ceramics. J Biomed Mater Res, 53(4), 304-313, 2000. https://doi.org/10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S
  16. Lee HH. A clinical consideration of current dental zirconia CAD/CAM restorations. The Journal of Korean Dental Association, 49(5), 279-285, 2011.
  17. Mecholsky JJ. Fractography: Determining the sites of fracture initiation. Dent Mater, 11(2), 113-116, 1995. https://doi.org/10.1016/0109-5641(95)80045-X
  18. Ozkurt Z, Kazazoglu E, Unal A. In vitro evaluation of shear bond strength of veneering ceramics to zirconia. Dent Mater J, 29(2), 138-146, 2010. https://doi.org/10.4012/dmj.2009-065
  19. Rosenblum MA, Schulman A. A review of allceramic restoration. JADA, 128(3), 297-307, 1997.
  20. Shin ES, Lee YS, Park WH. Comparative study in fracture strength of zirconia cores fabricated with three different CAD/CAM systems. J Korean Acad Prosthodont, 46(1), 22-30, 2008.
  21. Sorensen JA, Engelman MJ, Torres TJ, Avera SP. Shear bond strength of composite resin to porcelain. Int J Prosthodont, 4(1), 17-23, 1991.
  22. Sundh A, Sjogren G. A comparison of fracture strength of yttrium-oxide-partiallystabilized zirconia ceramic crowns with varying core thickness, shape and veneer ceramics. J Oral Rehabil, 31(7), 682-688, 2004. https://doi.org/10.1111/j.1365-2842.2004.01284.x
  23. Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H. Fracture resistance of lithium disilicate-, alumina-, and zirconiabased three unit fixed partial dentures: A laboratory study. Int J Prosthodont, 14(3), 231-238, 2001.
  24. Vagkopoulou T, Koutayas SO, Koidis P, Strub JR. Zirconia in dentistry: Part 1. Discovering the nature of an upcoming bioceramic. Eur J Esthet Dent, 4(2), 130-151, 2009.