Abstract
The objective of this study is to examine the fatigue behavior in compression of normal-weight and lightweight concrete mixtures with high volume supplementary cementitious material(SCM). The selected binder composition was 30% ordinary portland cement, 20% fly-ash, and 50% ground granulated blast-furnace slag. The targeted compressive strength of concrete was 40 MPa. For the cyclic loading, the constant maximum stress level varied to be 75%, 80%, and 90% of the static uniaxial compressive strength, whereas the constant minimum stress level was fixed at 10% of the static strength. The test results showed that fatigue life of high volume SCM lightweight concrete was lower than the companion normalweight concrete. The value of the fatigue strain at the maximum stress level intersected the descending branch of the monotonic stress-strain curve after approximately 90% of the fatigue life.
이 연구의 목적은 혼화재 다량 치환 경량 및 보통중량 콘크리트의 압축 피로 특성 평가이다. 사용된 결합재는 시멘트 30%, 플라이애쉬 20%, 고로슬래그 50%이다. 콘크리트의 설계 압축강도는 40MPa 이다. 반복하중은 최대 응력비가 정적 콘크리트 압축강도의 75%, 80% 및 90%와 최소 응력비가 정적 강도의 10% 범위에서 1Hz의 속도로 가력하였다. 실험결과 혼화재 다량 치환 경량콘크리트의 피로수명은 혼화재 다량치환 보통중량 콘크리트에 비해 다소 낮았다. 최대응력에서의 피로변형률 값은 피로수명의 약 90% 이후부터 정정 응력-변형률 곡선의 하강부와 교차하였다.