PURPOSE. This study evaluated the bond strength between porcelain denture teeth (Bioblend 43D) and four different polymerized denture resins (Lucitone 199, Palapress, Acron MC, Triad) with and without a bonding agent and after four different types of surface treatment (polished, HF etched, sandblasted, air-abraded). MATERIALS AND METHODS. Central incisor porcelain denture teeth were divided into 32 groups of 5 each. Tensile bond strength (MPa) was determined using a testing machine at crosshead speed of 0.5 mm/min. Mean and standard deviation are listed. Data were analyzed by two-way ANOVA. Means were compared by Tukey-Kramer intervals at 0.05 significance level. RESULTS. All surface treatment increased bond strength compared to polished surface and the highest bond strength was found with Palapress resin with etched porcelain surface (8.1 MPa). Bonding agent improved the bond strength of all denture resins to porcelain teeth. Superior bonding was found with Palapress and air-abraded porcelain (39 MPa). CONCLUSION. Resins with different curing methods affect the bond strength of porcelain teeth to denture bases. Superior bonding was found with auto-polymerized resin (Palapress). Application of ceramic primer and bonding agent to porcelain teeth with and without surface treatment will improve the bond strength of all denture resins to porcelain teeth.

키워드

참고문헌

  1. Buyukyilmaz S, Ruyter IE. The effects of polymerization temperature on the acrylic resin denture base-tooth bond. Int J Prosthodont 1997;10:49-54.
  2. Takahashi Y, Chai J, Takahashi T, Habu T. Bond strength of denture teeth to denture base resins. Int J Prosthodont 2000; 13:59-65.
  3. El-Sheikh MM, Powers JM. Tensile bond strength of porcelain teeth to denture resin before and after aging. Int J Prosthodont 1998;11:16-20.
  4. Craig RG. Prosthetic appliance of polymers. In: Restorative Dental Materials. 11th ed. St Louis: Mosby, 2002, p. 570-1.
  5. Spohr AM, Sobrinho LC, Consani S, Sinhoreti MA, Knowles JC. Influence of surface conditions and silane agent on the bond of resin to IPS Empress 2 ceramic. Int J Prosthodont 2003;16:277-82.
  6. Filho AM, Vieira LC, Araújo E, Monteiro Júnior S. Effect of different ceramic surface treatments on resin microtensile bond strength. J Prosthodont 2004;13:28-35. https://doi.org/10.1111/j.1532-849X.2004.04007.x
  7. Roulet JF, Soderholm KJ, Longmate J. Effects of treatment and storage conditions on ceramic/composite bond strength. J Dent Res 1995;74:381-7. https://doi.org/10.1177/00220345950740011501
  8. Kato H, Matsumura H, Atsuta M. Effect of etching and sandblasting on bond strength to sintered porcelain of unfilled resin. J Oral Rehabil 2000;27:103-10. https://doi.org/10.1046/j.1365-2842.2000.00489.x
  9. Yunus N, Harrison A, Huggett R. Effect of microwave irradiation on the flexural strength and residual monomer levels of an acrylic resin repair material. J Oral Rehabil 1994;21: 641-8.
  10. Schneider RL, Curtis ER, Clancy JM. Tensile bond strength of acrylic resin denture teeth to a microwave- or heat-processed denture base. J Prosthet Dent 2002;88:145-50. https://doi.org/10.1067/mpr.2002.127898
  11. Cunningham JL. Shear bond strength of resin teeth to heatcured and light-cured denture base resin. J Oral Rehabil 2000; 27:312-6. https://doi.org/10.1046/j.1365-2842.2000.00522.x
  12. Clancy JM, Hawkins LF, Keller JC, Boyer DB. Bond strength and failure analysis of light-cured denture resins bonded to denture teeth. J Prosthet Dent 1991;65:315-24. https://doi.org/10.1016/0022-3913(91)90182-V
  13. Jardel V, Degrange M, Picard B, Derrien G. Correlation of topography to bond strength of etched ceramic. Int J Prosthodont 1999;12:59-64.
  14. Ozcan M. A practical method for chairside repair of debonded porcelain denture teeth. J Prosthodont 2006;15:47-50. https://doi.org/10.1111/j.1532-849X.2006.00068.x
  15. Panah FG, Rezai SM, Ahmadian L. The influence of ceramic surface treatments on the micro-shear bond strength of composite resin to IPS Empress 2. J Prosthodont 2008;17: 409-14. https://doi.org/10.1111/j.1532-849X.2007.00296.x
  16. Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000;2:139-47.
  17. Marchack BW, Yu Z, Zhao XY, White SN. Adhesion of denture tooth porcelain to heat-polymerized denture resin. J Prosthet Dent 1995;74:242-9. https://doi.org/10.1016/S0022-3913(05)80130-1