DOI QR코드

DOI QR Code

Effect of various intraoral repair systems on the shear bond strength of composite resin to zirconia

  • Han, In-Hae (Department of Prosthodontics, School of Dentistry, Chosun University) ;
  • Kang, Dong-Wan (Department of Prosthodontics, School of Dentistry, Chosun University) ;
  • Chung, Chae-Heon (Department of Prosthodontics, School of Dentistry, Chosun University) ;
  • Choe, Han-Cheol (Department of Dental Materials, School of Dentistry, Chosun University) ;
  • Son, Mee-Kyoung (Department of Prosthodontics, School of Dentistry, Chosun University)
  • Received : 2012.12.11
  • Accepted : 2013.06.21
  • Published : 2013.08.31

Abstract

PURPOSE. This study compared the effect of three intraoral repair systems on the bond strength between composite resin and zirconia core. MATERIALS AND METHODS. Thirty zirconia specimens were divided into three groups according to the repair method: Group I-CoJet$^{TM}$ Repair System (3M ESPE) [chairside silica coating with $30{\mu}m$ $SiO_2$ + silanization + adhesive]; Group II-Ceramic Repair System (Ivoclar Vivadent) [etching with 37% phosphoric acid + Zirconia primer + adhesive]; Group III-Signum Zirconia Bond (Heraus) [Signum Zirconia Bond I + Signum Zirconia Bond II]. Composite resin was polymerized on each conditioned specimen. The shear bond strength was tested using a universal testing machine, and fracture sites were examined with FE-SEM. Surface morphology and wettability after surface treatments were examined additionally. The data of bond strengths were statistically analyzed with one-way ANOVA and Tamhane post hoc test (${\alpha}$=.05). RESULTS. Increased surface roughness and the highest wettability value were observed in the CoJet sand treated specimens. The specimens treated with 37% phosphoric acid and Signum Zirconia Bond I did not show any improvement of surface irregularity, and the lowest wettability value were found in 37% phosphoric acid treated specimens. There was no significant difference in the bond strengths between Group I ($7.80{\pm}0.76$ MPa) and III ($8.98{\pm}1.39$ MPa). Group II ($3.21{\pm}0.78$ MPa) showed a significant difference from other groups (P<.05). CONCLUSION. The use of Intraoral silica coating system and the application of Signum Zirconia Bond are effective for increasing the bond strength of composite resin to zirconia.

Keywords

References

  1. Choi BK, Han JS, Yang JH, Lee JB, Kim SH. Shear bond strength of veneering porcelain to zirconia and metal cores. J Adv Prosthodont 2009;1:129-35. https://doi.org/10.4047/jap.2009.1.3.129
  2. Jang GW, Kim HS, Choe HC, Son MK. Fracture strength and mechanism of dental ceramic crown with zirconia thickness. Procedia Eng 2011;10:1556-60.
  3. Ural C, Kulunk T, Külünk S, Kurt M, Baba S. Determination of resin bond strength to zirconia ceramic surface using different primers. Acta Odontol Scand 2011;69:48-53. https://doi.org/10.3109/00016357.2010.517558
  4. Chaiyabutr Y, McGowan S, Phillips KM, Kois JC, Giordano RA. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic. J Prosthet Dent 2008;100:194-202. https://doi.org/10.1016/S0022-3913(08)60178-X
  5. Thompson JY, Stoner BR, Piascik JR, Smith R. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now? Dent Mater 2011;27:71-82. https://doi.org/10.1016/j.dental.2010.10.022
  6. Triwatana P, Nagaviroj N, Tulapornchai C. Clinical performance and failures of zirconia-based fixed partial dentures: a review literature. J Adv Prosthodont 2012;4:76-83. https://doi.org/10.4047/jap.2012.4.2.76
  7. Ural C, Kulunk T, Kulunk S, Kurt M. The effect of laser treatment on bonding between zirconia ceramic surface and resin cement. Acta Odontol Scand 2010;68:354-9. https://doi.org/10.3109/00016357.2010.514720
  8. Kim BK, Bae HE, Shim JS, Lee KW. The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials. J Prosthet Dent 2005;94:357-62. https://doi.org/10.1016/j.prosdent.2005.08.012
  9. Cho HY, Won HY, Choe HC, Son MK. Fracture characteristics of dental ceramic crown according to zirconia coping design. Procedia Eng 2011;10:1561-6. https://doi.org/10.1016/j.proeng.2011.04.261
  10. Hatta M, Shinya A, Yokoyama D, Gomi H, Vallittu PK, Shinya A. The effect of surface treatment on bond strength of layering porcelain and hybrid composite bonded to zirconium dioxide ceramics. J Prosthodont Res 2011;55:146-53. https://doi.org/10.1016/j.jpor.2010.10.005
  11. Choi YS, Kim SH, Lee JB, Han JS, Yeo IS. In vitro evaluation of fracture strength of zirconia restoration veneered with various ceramic materials. J Adv Prosthodont 2012;4:162-9. https://doi.org/10.4047/jap.2012.4.3.162
  12. Casucci A, Monticelli F, Goracci C, Mazzitelli C, Cantoro A, Papacchini F, Ferrari M. Effect of surface pre-treatments on the zirconia ceramic-resin cement microtensile bond strength. Dent Mater 2011;27:1024-30. https://doi.org/10.1016/j.dental.2011.07.002
  13. Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Selective infiltration- etching technique for a strong and durable bond of resin cements to zirconia-based materials. J Prosthet Dent 2007; 98:379-88. https://doi.org/10.1016/S0022-3913(07)60123-1
  14. Sailer I, Feher A, Filser F, Luthy H, Gauckler LJ, Scharer P, Franz Hammerle CH. Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up. Quintessence Int 2006;37:685-93.
  15. Sailer I, Feher A, Filser F, Gauckler LJ, Luthy H, Hammerle CH. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont 2007;20:383-8.
  16. Wataha JC. Alloys for prosthodontic restorations. J Prosthet Dent 2002;87:351-63. https://doi.org/10.1067/mpr.2002.123817
  17. Fischer J, Baltzer N, Fleetwood PW. Thermal creep analysis of noble metal alloys for the ceramic-fused-to-metal technique. J Biomed Mater Res 1999;48:258-64. https://doi.org/10.1002/(SICI)1097-4636(1999)48:3<258::AID-JBM9>3.0.CO;2-K
  18. Anusavice KJ, Carroll JE. Effect of incompatibility stress on the fit of metal-ceramic crowns. J Dent Res 1987;66:1341-5. https://doi.org/10.1177/00220345870660081101
  19. Della Bona A, Borba M, Benetti P, Cecchetti D. Effect of surface treatments on the bond strength of a zirconia-reinforced ceramic to composite resin. Braz Oral Res 2007;21:10-5. https://doi.org/10.1590/S1806-83242007000100002
  20. Park JS, Kim HS, Kim HSL, Song MK, Choe HC. Interfacial Bonding and Fracture Phenomena between Porcelain and Metal Coping. Procedia Eng 2011;10:1567-72. https://doi.org/10.1016/j.proeng.2011.04.262
  21. Son MK, Choe HC. Evaluation of Interfacial Bonding Strength between Laser Textured Metal Coping and Porcelain. Procedia Eng 2011;10:2268-91.
  22. Qeblawi DM, Munoz CA, Brewer JD, Monaco EA Jr. The effect of zirconia surface treatment on flexural strength and shear bond strength to a resin cement. J Prosthet Dent 2010; 103:210-20. https://doi.org/10.1016/S0022-3913(10)60033-9
  23. Yang B, Wolfart S, Scharnberg M, Ludwig K, Adelung R, Kern M. Influence of contamination on zirconia ceramic bonding. J Dent Res 2007;86:749-53. https://doi.org/10.1177/154405910708600812
  24. Zhang Y, Lawn BR, Malament KA, Van Thompson P, Rekow ED. Damage accumulation and fatigue life of particle-abraded ceramics. Int J Prosthodont 2006;19:442-8.
  25. Zhang Y, Lawn BR, Rekow ED, Thompson VP. Effect of sandblasting on the long-term performance of dental ceramics. J Biomed Mater Res B Appl Biomater 2004;71:381-6.
  26. Gokce B, Ozpinar B, Dundar M, Comlekoglu E, Sen BH, Gungor MA. Bond strengths of all-ceramics: acid vs laser etching. Oper Dent 2007;32:173-8. https://doi.org/10.2341/06-52
  27. Fischer J, Grohmann P, Stawarczyk B. Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites. Dent Mater J 2008;27:448-54. https://doi.org/10.4012/dmj.27.448
  28. Matinlinna JP, Lassila LV, Vallittu PK. The effect of a novel silane blend system on resin bond strength to silica-coated Ti substrate. J Dent 2006;34:436-43. https://doi.org/10.1016/j.jdent.2005.09.007
  29. Blatz MB, Sadan A, Martin J, Lang B. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling. J Prosthet Dent 2004;91:356-62. https://doi.org/10.1016/j.prosdent.2004.02.001
  30. Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000;2:139-47.
  31. Ersu B, Yuzugullu B, Ruya Yazici A, Canay S. Surface roughness and bond strengths of glass-infiltrated alumina-ceramics prepared using various surface treatments. J Dent 2009;37: 848-56. https://doi.org/10.1016/j.jdent.2009.06.017
  32. Valandro LF, Ozcan M, Amaral R, Vanderlei A, Bottino MA. Effect of testing methods on the bond strength of resin to zirconia-alumina ceramic: microtensile versus shear test. Dent Mater J 2008;27:849-55. https://doi.org/10.4012/dmj.27.849
  33. Chadwick RG, Mason AG, Sharp W. Attempted evaluation of three porcelain repair systems-what are we really testing? J Oral Rehabil 1998;25:610-5. https://doi.org/10.1046/j.1365-2842.1998.00283.x
  34. Lindgren J, Smeds J, Sjogren G. Effect of surface treatments and aging in water on bond strength to zirconia. Oper Dent 2008;33:675-81. https://doi.org/10.2341/08-12

Cited by

  1. Comparison of the Effectiveness of Bonding Composite to Zirconia as a Repair Method vol.13, pp.2, 2015, https://doi.org/10.1111/ijac.12498
  2. Surface Treatments for Repair of Feldspathic, Leucite - and Lithium Disilicate-Reinforced Glass Ceramics Using Composite Resin vol.26, pp.2, 2015, https://doi.org/10.1590/0103-6440201302447
  3. In Vitro Comparison of the Bond Strength between Ceramic Repair Systems and Ceramic Materials and Evaluation of the Wettability vol.26, pp.3, 2015, https://doi.org/10.1111/jopr.12381
  4. Repair bond strength of composite resin to sandblasted and laser irradiated Y-TZP ceramic surfaces vol.37, pp.3, 2015, https://doi.org/10.1002/sca.21197
  5. Efficacy of ceramic repair material on the bond strength of composite resin to zirconia ceramic vol.73, pp.1, 2015, https://doi.org/10.3109/00016357.2014.946963
  6. Structural and Chemical Characterization of Silica Spheres before and after Modification by Silanization for Trypsin Immobilization vol.2017, pp.1687-4129, 2017, https://doi.org/10.1155/2017/1610597
  7. Fracture resistance of zirconia-composite veneered crowns in comparison with zirconia-porcelain crowns vol.36, pp.3, 2017, https://doi.org/10.4012/dmj.2016-298
  8. Intraoral repair of chipped or fractured veneered zirconia crowns and fixed dental prosthesis: clinical guidelines based on literature review vol.32, pp.15, 2018, https://doi.org/10.1080/01694243.2018.1443639
  9. Can low-fusing glass application affect the marginal misfit and bond strength of Y-TZP crowns? vol.32, pp.0, 2018, https://doi.org/10.1590/1807-3107bor-2018.vol32.0034
  10. Zirconia Primers Improve the Shear Bond Strength of Dental Zirconia pp.1059941X, 2020, https://doi.org/10.1111/jopr.13013
  11. Influence of different surface treatments on microshear bond strength of repair resin composite to two CAD/CAM esthetic restorative materials vol.12, pp.3, 2015, https://doi.org/10.1016/j.tdj.2015.06.001
  12. Bond Strength of Zirconia to Different Core Materials vol.7, pp.4, 2016, https://doi.org/10.5005/jp-journals-10015-1389
  13. Bond Strength of Zirconia to Different Core Materials vol.7, pp.4, 2016, https://doi.org/10.5005/jp-journals-10015-1389
  14. Oxygen Plasma Improved Shear Strength of Bonding between Zirconia and Composite Resin vol.10, pp.7, 2013, https://doi.org/10.3390/coatings10070635
  15. Fractured zirconia restorations repair bonding durability using two different adhesives vol.18, pp.4, 2013, https://doi.org/10.4103/tdj.tdj_5_21
  16. Evaluation of Efficacy of Various Surface Conditioning Methods on the Repair Bond Strength of Composite to Different Fracture Types of Zirconia Ceramics vol.2021, pp.None, 2013, https://doi.org/10.1155/2021/5537761
  17. Effect of Air-Abraded Versus Laser-Fused Fluorapatite Glass-Ceramics on Shear Bond Strength of Repair Materials to Zirconia vol.14, pp.6, 2013, https://doi.org/10.3390/ma14061468
  18. Shear Bond Strength of Veneered Zirconia Repaired Using Various Methods and Adhesive Systems: A Comparative Study vol.13, pp.6, 2013, https://doi.org/10.3390/polym13060910
  19. Cold Atmospheric Plasma Improves Shear Bond Strength of Veneering Composite to Zirconia vol.9, pp.6, 2013, https://doi.org/10.3390/dj9060059
  20. Do Chemical-Based Bonding Techniques Affect the Bond Strength Stability to Cubic Zirconia? vol.14, pp.14, 2013, https://doi.org/10.3390/ma14143920
  21. Effects of laser modalities on shear bond strengths of composite superstructure to zirconia and PEEK infrastructures: an in vitro study vol.109, pp.4, 2013, https://doi.org/10.1007/s10266-021-00608-1