Humidity Induced Defect Generation and Its Control during Organic Bottom Anti-reflective Coating in the Photo Lithography Process of Semiconductors

  • Mun, Seong-Yeol (Department of Foundries FAB, Globalfoundries Silicon Partners Pte. Ltd.) ;
  • Kang, Seong-Jun (Department of Electrical and Semiconductor Engineering, Chonnam National University) ;
  • Joung, Yang-Hee (Department of Electrical and Semiconductor Engineering, Chonnam National University)
  • Received : 2012.05.09
  • Accepted : 2012.06.05
  • Published : 2012.09.30

Abstract

Defect generation during organic bottom anti-reflective coating (BARC) in the photo lithography process is closely related to humidity control in the BARC coating unit. Defects are related to the water component due to the humidity and act as a blocking material for the etching process, resulting in an extreme pattern bridging in the subsequent BARC etching process of the poly etch step. In this paper, the lower limit for the humidity that should be stringently controlled for to prevent defect generation during BARC coating is proposed. Various images of defects are inspected using various inspection tools utilizing optical and electron beams. The mechanism for defect generation only in the specific BARC coating step is analyzed and explained. The BARC defect-induced gate pattern bridging mechanism in the lithography process is also well explained in this paper.

Keywords

References

  1. F. Yeung and Y. C. Chan, "Electrical failure of multilayer ceramic capacitors caused by high temperature and high humidity environment," Proceedings of the 44th Electronic Components and Technology Conference, Washington, DC, pp. 847-853, 1994.
  2. H. C. Ling and A. M. Jackson, "Correlation of silver migration with temperature-humidity-bias (THB) failures in multilayer ceramic capacitors," IEEE Transactions on Components, Hybrids, and Manufacturing Technology, vol. 12, no. 1, pp. 130-137, 1989. https://doi.org/10.1109/33.19027
  3. S. Luo and C. P. Wong, "Study on influence of environment on adhesion performance of underfill for flip chip application," Proceedings of International Symposium on Electronic Materials and Packaging, Hong Kong, pp. 243-250, 2000.
  4. J. C. W. van Vroonhoven, "Effects of adhesion and delamination on stress singularities in plastic-packaged integrated circuits," Journal of Electronic Packaging, vol. 115, no. 1, pp. 28-33, 1993. https://doi.org/10.1115/1.2909298
  5. J. V. Champion and S. J. Dodd, "The effect of absorbed water on electrical treeing in epoxy resins," Proceedings of the 7th International Conference on Dielectric Materials, Measurements and Applications, Bath, UK, pp. 206-210, 1996.
  6. M. W. Lane, X. H. Liu, and T. M. Shaw, "Environmental effects on cracking and delamination of dielectric films," IEEE Transactions on Device and Materials Reliability, vol. 4, no. 2, pp. 142-147, 2004. https://doi.org/10.1109/TDMR.2004.829123
  7. X. H. Liu, T. M. Shaw, M. W. Lane, R. R. Rosenberg, S. L. Lane, J. P. Doyle, D. Restaino, S. F. Vogt, and D. C. Edelstaeing, "Channel cracking in low-k films on patterned multi-layers," Proceedings of the IEEE International Interconnect Technology Conference, Burlingame, CA, pp. 93-95, 2004.
  8. C. J. Neef, J. Finazzo, C. Nesbit, and M. Weigand, "Effects of bake temperature and surface modifications on hardmask materials for trilayer applications," Proceedings of the SPIE, vol. 6923, pp. 692331, 2008.

Cited by

  1. Review-Airborne Molecular Contamination: Recent Developments in the Understanding and Minimization for Advanced Semiconductor Device Manufacturing vol.9, pp.6, 2012, https://doi.org/10.1149/2162-8777/aba080
  2. Flow analysis of a front opening unified pod (FOUP) subjected to different fan filter unit (FFU) coverage area in mini-environment vol.12, pp.None, 2012, https://doi.org/10.1016/j.ijft.2021.100124