Early-Age Shrinkage and Durability of Shotcrete with Expansive Agent

팽창재를 혼입한 숏크리트의 초기수축 및 내구성 평가

  • Received : 2012.03.20
  • Accepted : 2012.10.11
  • Published : 2012.10.31

Abstract

In this dissertation, the shrinkage and durability of shotcrete were examined. Analysis and comparison of shrinkage against the strength of shotcrete was investigated after performing actual shotcrete shooting for each mix of different percentage of expansive agent. The research on restrained shrinkage with different percentages of expansive agent used (3%, 7%, 11% and 15%) shows that the maximum shrinkage in all samples occurred in between 13-15 hrs after shotcrete shooting. And it is noticed that increasing the percentage of expansive agent can lower the shrinkage. And hence, the 15% of expansive agent not only lowered the shrinkage But it also lowered the strength.

본 논문에서는 숏크리트의 품질확보를 위하여 숏크리트에 팽창재 혼입률의 변동을 주어 혼입하여 숏크리트의 초기수축과 기초적인 내구성에 미치는 영향을 고찰하였다. 또한 각각의 팽창제 혼입률에 따라 실제 숏크리트 타설을 실시한 후 숏크리트 초기수축을 비교 분석하였으며 내구성에 대하여 고찰하였다. 시험을 실시한 모든 변수에서 타설 13~15시간 후 최대 수축이 발생하였고, 팽창재의 혼입률을 높일수록 최대수축량이 줄어듬을 알 수 있었다. 이는 급결제를 사용하지 않는 건축물 숏크리트에 참고자료로 활용될 수 있다고 판단된다. 또한 팽창재의 혼입률의 경우 시멘트 대비 15%일 때는 최대수축량은 작지만 수축과 팽창이 급격히 이루어져 미세균열에 심각하게 노출될 염려가 있으므로 11%가 적당하다 판단된다.

Keywords

References

  1. Shim, Hyun-Bo, A Experimental Study on the Drying Shrinkage Characteristic of Concrete with Expensive Additives, Kon-Kuk University, 2000
  2. Park, Sun-Gyu, Study on the Autogenous Shrinkage Prediction of High Strength Concrete using Shrinkage Reducing Admixture, Journal of the Architectural Institute of Korea, 2008
  3. Wen, Xue Long, Engineering Properties of High Performance Concrete with the Combination of Expansive Additive and Shrinkage Reducing Agent, Chongju University, 2004
  4. Hong, Sang-hee, Jun, Byung-Chea, Song, Myong-Shin, Han, Cheon-Goo, Bahn, Ho-Yong, An Experimental Study on the reduction of High Drying and Autogenous Shrinkage of High Performance Concrete Using CSA Expansive Additives, Journal of the Architectural Institute of Korea, 1998
  5. ASTM C1202-91 "Electrical indication of concrete stability to resist chloride ion penetration"