Abstract
An orthogonal magnetic field is often used for a military vessel in the deperm process such as Flash D deperm protocol and Anhysteretic deperm protocol. The effect of the orthogonal magnetic field on a deperm performance was investigated for a sample with strain-induced magnetization and field-induced magnetization given to different direction. A 70mm wide, 110mm long and 0.25mm thick rectangular steel plate was bent to have U-shape and to generate a strong strain on the bottom region of U-shaped steel plate. Field-induced magnetization was attached by NdFeB permanent magnet. Demagnetization was performed by applying magnetic field with a step decrement from the first field(the first shot) under the action of DC bias field.