초록

Cast iron pipe has been used as a water distribution technology in North America since the early nineteenth century. The first cast iron pipes were made of grey cast iron which was succeeded by ductile iron as a pipe material in the 1940s. These different iron alloys have significantly different microstructures which give rise to distinct mechanical properties. Insight into the non-destructive structural condition assessment of aging pipes can be advantageous in developing mitigation strategies for pipe failures. This paper examines the relationship between the small-strain and large-strain properties of exhumed cast iron water pipes. Nondestructive and destructive testing programs were performed on eight pipes varying in age from 40 to 130 years. The experimental program included microstructure evaluation and ultrasonic, tensile, and flexural testing. New applications of frequency domain analysis techniques including Fourier and wavelet transforms of ultrasonic pulse velocity measurements are presented. A low correlation between wave propagation and large-strain measurements was observed. However, the wave velocities were consistently different between ductile and grey cast iron pipes (14% to 18% difference); the ductile iron pipes showed the smaller variation in wave velocities. Thus, the variation of elastic properties for ductile iron was not enough to define a linear correlation because all the measurements were practically concentrated in single cluster of points. The cross-sectional areas of the specimens tested varied as a result of minor manufacturing defects and levels of corrosion. These variations affect the large strain testing results; but, surface defects have limited effect on wave velocities and may also contribute to the low correlations observed. Lamb waves are typically not considered in the evaluation of ultrasonic pulse velocity. However, Lamb waves were found to contribute significantly to the frequency content of the ultrasonic signals possibly resulting in the poor correlations observed. Therefore, correlations between wave velocities and large strain properties obtained using specimens manufactured in the laboratory must be used with caution in the condition assessment of aged water pipes especially for grey cast iron pipes.

키워드

참고문헌

  1. Abdel-Megeed, S.M. (1984), "Accuracy of correlation coefficient with limited number of points", J. Exp. Educ., 52(4), 188-191. https://doi.org/10.1080/00220973.1984.11011891
  2. Angus, H.T. (1976), Cast Iron: Physical and Engineering Properties, Toronto, Butterworth & Co. Inc.
  3. ASTM Standard D790 - 07 (2007), Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials, ASTM International, West Conshohocken.
  4. ASTM Standard E8/E8M - 08 (2008), Standard Methods for Tension Testing of Metallic Materials. ASTM International, West Conshohocken, PA.
  5. Bilgin, O. and Stewart, H. (2009), "Pullout resistance characteristics of cast iron pipe", J. Transport. Eng., 135(10), 730-735. https://doi.org/10.1061/(ASCE)0733-947X(2009)135:10(730)
  6. Blitz, J. and Simpson, G. (1996), Ultrasonic Methods of Non-Destructive Testing, Chapman & Hall, New York.
  7. Bracewell, R. (2007), The Fourier Transform and its Applications, McGraw-Hill, New York.
  8. Cammarata, M., Rizzo, P., Dutta, D. and Sohn, H. (2010), "Application of principal component analysis and wavelet transform to fatigue crack detection in waveguides", Smart Struct. Syst., 6(4), 349-362. https://doi.org/10.12989/sss.2010.6.4.349
  9. Collins, D. and Alchekh, W. (1995), "Ultrasonic non-destructive evaluation of the matrix structure and the graphite shape in cast iron", J. Mater. Process. Tech., 55(2), 85-90 https://doi.org/10.1016/0924-0136(95)01789-5
  10. Davis, J.R. (1996), Cast Irons, ASM International, Materials Park, OH.
  11. Fuller, A., Emerson, P. and Sergeant, G. (1990), "A report on the effect upon mechanical properties of variation in graphite form in irons having varying amounts of ferrite and pearlite in the matrix structure and the use of nondestructive tests in the assessments of mechanical properties of such irons", AFS Transactions, 88, 21-50.
  12. Graff, K. (1991), Wave motion in elastic solids, Dover Publications Inc., New York.
  13. Gokdag, H. and Kopmaz, O. (2010), "A new structural damage detection index based on analyzing vibration modes by the wavelet transform", Struct. Eng. Mech., 35(2), 257-260. https://doi.org/10.12989/sem.2010.35.2.257
  14. Karsay, S.I. (1970), Ductile Iron II Engineering Design Properties Applications, Quebec Iron and Titanium Corporation, Sorel, QC.
  15. Khan, Z., Cascante, G. and El Naggar, M.H. (2007), "Measurement of dynamic properties of a cemented sand using ultrasonic waves", Can. Geotech. J. (in print)
  16. Koelble, F.T. (2006), Cast Iron Soil Pipe Fittings Handbook, Cast Iron Soil Pipe Institute, Washington, DC.
  17. Lee, S.Y., Rus, G. and Park, T. (2008), "Quantitative nondestructive evaluation of thin plate structures using the complete frequency information from impact testing", Struct. Eng. Mech., 28(5), 525-548. https://doi.org/10.12989/sem.2008.28.5.525
  18. Lu, Y., Ye, L., Wang, D., Zhou, L. and Cheng, L. (2010), "Piezo-activated guided wave propagation and interaction with damage in tubular structures", Smart Struct. Syst., 6(7), 835-849. https://doi.org/10.12989/sss.2010.6.7.835
  19. Makar, J.M. and Rajani, B. (2000), "Gray cast-iron water pipe metallurgy", J. Mat. Civil Eng., 12(3), 245-253. https://doi.org/10.1061/(ASCE)0899-1561(2000)12:3(245)
  20. Ohide, T., Ohira, G. and Ikawa, K. (1989), "Evaluation of mechanical properties of cast iron by ultrasonic velocity", Proceedings of the Physical Metallurgy of Cast Iron IV, Tokyo, Japan, September.
  21. Orlowicz, W., Tupaja, M., Mróza, M. and Guzikb, E. (2010), "Evaluation of ductile iron casting material quality using ultrasonic testing", J. Mater. Process. Tech., 210(11), 1493-1500. https://doi.org/10.1016/j.jmatprotec.2010.04.007
  22. Rajani, B. (2000), Investigation of Grey Cast Iron Water Mains to Develop a Methodology for Estimating ServiceLife, American Water Works Association Research Foundation, USA.
  23. Seica, M.V. and Packer, J.A. (2004), "Mechanical properties and strength of aged cast iron water pipes", J. Mat.Civil Eng., 16(1), 69-77. https://doi.org/10.1061/(ASCE)0899-1561(2004)16:1(69)
  24. Skabo, R. and Jackson, R. (1991), Nondestructive testing of water mains for physical integrity, CH2M Hill Technical Report, USA.
  25. Tamburelli, C. and Quaroni, A. (1975), "Ultrasonic velocity measurement to inspect malleable iron castings", Non-Destruct. Test., 8(3), 152-157. https://doi.org/10.1016/0029-1021(75)90025-0
  26. Walton, C.F. (1971), Gray and Ductile Iron Casting Handbook, Gray and Ductile Iron Founders' Society Inc., Cleveland, OH.