청자 유약 발색메카니즘에 대한 뫼스바우어 분광법에 의한 연구

Mössbauer Spectroscopic Study on Colorative Mechanism of Celadon Glaze

  • 김종영 (한국세라믹기술원 이천분원) ;
  • 노형구 (한국세라믹기술원 이천분원) ;
  • 전아영 (한국세라믹기술원 이천분원) ;
  • 김응수 (한국세라믹기술원 이천분원) ;
  • 조우석 (한국세라믹기술원 이천분원) ;
  • 김경자 (한국세라믹기술원 이천분원) ;
  • 김진모 (국민대학교 물리학과) ;
  • 김철성 (국민대학교 물리학과)
  • Kim, Jong-Young (Icheon Branch, Korea Institute of Ceramic Engineering and Technology) ;
  • No, Hyung-Goo (Icheon Branch, Korea Institute of Ceramic Engineering and Technology) ;
  • Jeon, A-Young (Icheon Branch, Korea Institute of Ceramic Engineering and Technology) ;
  • Kim, Ung-Soo (Icheon Branch, Korea Institute of Ceramic Engineering and Technology) ;
  • Cho, Woo-Seok (Icheon Branch, Korea Institute of Ceramic Engineering and Technology) ;
  • Kim, Kyung-Ja (Icheon Branch, Korea Institute of Ceramic Engineering and Technology) ;
  • Kim, Chin-Mo (Department of Physics, Kookmin University) ;
  • Kim, Chul-Sung (Department of Physics, Kookmin University)
  • 투고 : 2010.10.15
  • 심사 : 2010.11.17
  • 발행 : 2011.01.31

초록

Systematic study on relationship between celadon coloring and glaze component was conducted by chromaticity analysis and M$\ddot{o}$ssbauer spectroscopic analysis. The chromaticity ($L^*$, $a^*$, $b^*$ values) and M$\ddot{o}$ssbauer analysis results were correlated to the amount of $Fe_2O_3$, $TiO_2$, MnO, and $P_2O_5$, which are the essential factors influencing celadon coloring. According to chromaticity analysis, celadon glaze color belongs to GY group when the addition of $TiO_2$ was 1.4%, whereas the color belongs to BG group when the addition of $TiO_2$ was 0.1%. For the GY group, the colors change from GY to YR with the decrease of brightness as the addition of $TiO_2$, MnO, and $P_2O_5$ increases. According to M$\ddot{o}$ssbauer analysis results, as the amount of divalent iron ion increases, the $a^*$ and $b^*$ values decrease, on the other hand, $L^*$ value increases. The ratio of divalent iron ion produced in reductive sintering process is found to be 80~95% in this study, which induces the increase of $L^*$ values in celadon glaze.

키워드

참고문헌

  1. Y. I. Yoon, "The Beauty of Ancient Korean Porcelains," pp. 202-243 Dolbegae press, 2007.
  2. Y. M. Jeong, "Goryo Celadon," pp.21-97, Daewonsa, 1998.
  3. Y. Yang, M. Feng, X. Ling, Z. Mao, C. Wang, X. Sun, and M. Guo, "Microstructural Analysis of the Color-generating Mechanism in Ru Ware, Modern Copies and its Differentiation with Jun Ware," J. Archaeological Science, 32 301-10 (2005). https://doi.org/10.1016/j.jas.2004.09.007
  4. G. Zhengyao, C. Songhua, and C. Xiande, "Mossbauer Study of the Ru Porcelain of Chinese Song Dynasty and Yuan Dynasty," Hyperfine Interactions, 91 663-68 (1994). https://doi.org/10.1007/BF02064587
  5. B. Zhang, Y.L. Liu, Z.Y. Gao, W.J. Zhao, G.X. Li, and H.S. Cheng, "Mossbauer Spectroscopy, NAA and PIXE Study on Some Archaeological Problems of Ancient Chinese Ru Celadon," Hyperfine Interactions, 163 1-12 (2005).
  6. Z. Bin and G. Zhengyao, "NAA and Mossbauer Study on Colorative Mechanism of Yaozhou Celadon in Ancient China," Hyperfine Interactions, 142 593-99 (2002). https://doi.org/10.1023/A:1022422117357

피인용 문헌

  1. Reaction Iron Oxide and Magnesium Oxide in Ceramics Body with Glaze vol.24, pp.7, 2014, https://doi.org/10.3740/MRSK.2014.24.7.363