Hydrogen Embrittlement Evaluation of Subsurface Zone in 590DP Steel by Micro-Vickers Hardness Measurement

미소경도 측정에 의한 590DP강 Subsurface Zone 내 수소취성 평가

  • Choi, Jong-Un (Department of Materials Science and Engineering, Seoul National University of Science and Technology) ;
  • Park, Jae-Woo (Department of Materials Science and Engineering, Seoul National University of Science and Technology) ;
  • Kang, Kae-Myung (Department of Materials Science and Engineering, Seoul National University of Science and Technology)
  • 최종운 (서울과학기술대학교 신소재공학과) ;
  • 박재우 (서울과학기술대학교 신소재공학과) ;
  • 강계명 (서울과학기술대학교 신소재공학과)
  • Received : 2011.09.05
  • Accepted : 2011.10.15
  • Published : 2011.11.27

Abstract

This study describes a hydrogen embrittlement evaluation of the subsurface zone in 590DP steel by micro-Vickers hardness measurement. The 590DP steel was designed to use in high-strength thin steel sheets as automotive materials. The test specimens were fabricated to 5 series varying the chemical composition through the process of casting and rolling. Electrochemical hydrogen charging was conducted on each specimen with varying current densities and charging times. The relationship between the embrittlement and hydrogen charging conditions was established by investigating the metallography. The micro-Vickers hardness was measured to evaluate the hydrogen embrittlement of the subsurface zone in addition to the microscopic investigation. The micro-Vickers hardness increased with the charging time at the surface. However, the changing ratio and maximum variation of hardness with depth were nearly the same value for each test specimen under the current density of 150 mA/$cm^2$ and charging time of 50 hours. Consequently, it appears that hydrogen embrittlement in 590DP steel can be evaluated by micro-Vickers hardness measurement.

Keywords

References

  1. R. P. Gangloff and R. P. Wei, Metall. Mater. Trans., 8A, 1043 (1977). https://doi.org/10.1007/BF02667388
  2. D. P. Williams and H. G. Nelson, Metall. Mater. Trans., 1B, 63 (1970).
  3. H. G. Nelson, D. P. Williams and A. S. Tetelmen, Metall. Mater. Trans., 2B, 953 (1971). https://doi.org/10.1007/BF02664224
  4. I. Maroef, D. L. Olson, M. Eberhart and G. R, Edwards, Int. Mater. Rev., 47(4), 191 (2002). https://doi.org/10.1179/095066002225006548
  5. J. P. Hirth, Metall. Mater. Trans., 11A, 861 (1980).
  6. W. Y. Choo and J. Y. Lee, Metall. Mater. Trans., 13A, 135 (1982). https://doi.org/10.1007/BF02642424
  7. T. Kushida, H. Matsumoto, N. Kuratomi, T. Tsumura, F. Nakasato and T. Kudo, Tetsu-to-Hagane, 82, 297 (1996) (in Japanese).
  8. R. G. Davies, Metall. Mater. Trans., 12A, 1667 (1981). https://doi.org/10.1007/BF02643572
  9. J. W. Park and K. M. Kang, Kor. J. Mater. Res., 20(11), 581 (2010) (in Korean). https://doi.org/10.3740/MRSK.2010.20.11.581
  10. J. W. Park and K. M. Kang, J. KIGAS, 14(6), 38 (2010) (in Korean).
  11. Y. H. Kim and J. W. Morris, Metall. Mater. Trans., 14A, 1883 (1983).
  12. K. Yokoyama, M. Tomita and J. Sakai, Acta Mater., 57, 1875 (2009). https://doi.org/10.1016/j.actamat.2008.12.030

Cited by

  1. The Effect of Hydrogen in Automobile High Strength Steel Sheets Charged with Hydrogen by Using Electrochemical Method vol.45, pp.5, 2012, https://doi.org/10.5695/JKISE.2012.45.5.212
  2. The Effect of Hydrogen on the Variation of Properties at the Surface Layers of 590 MPa DP Steels Charged with Hydrogen vol.46, pp.3, 2013, https://doi.org/10.5695/JKISE.2013.46.3.126
  3. An Analysis of Small Punch Test Conducted with the High Strength Dual Phase Sheet Steels Charged with Hydrogen vol.46, pp.5, 2013, https://doi.org/10.5695/JKISE.2013.46.5.229
  4. Analysis of Correlation between the Hydrogen Embrittlement and the Small Punch Test for Hydrogen-charged Dual Phase Steels vol.18, pp.1, 2014, https://doi.org/10.7842/kigas.2014.18.1.61
  5. Nanoindenter Test of 680MPa Dual Phase Steel Charged with Hydrogen vol.47, pp.1, 2014, https://doi.org/10.5695/JKISE.2014.47.1.033
  6. Small Punch Test of TRIP Steel Charged with Hydrogen under Different Electrolyte Condition vol.19, pp.1, 2015, https://doi.org/10.7842/kigas.2015.19.1.64