DOI QR코드

DOI QR Code

Color Enhancement for Cubic Zirconia with Low Temperature Annealing

큐빅지르코니아의 색향상을 위한 저온열처리 공정 연구

  • Li, Feng (Dept of Materials Science and Engineering, University of Seoul) ;
  • Shen, Yun (Dept of Materials Science and Engineering, University of Seoul) ;
  • Song, Oh-Sung (Dept of Materials Science and Engineering, University of Seoul)
  • 이봉 (서울시립대학교 신소재공학과) ;
  • 신운 (서울시립대학교 신소재공학과) ;
  • 송오성 (서울시립대학교 신소재공학과)
  • Received : 2009.12.11
  • Accepted : 2010.04.09
  • Published : 2010.04.30

Abstract

Colored cubic zirconia specimen made by skull melt process were annealed in vacuum at the temperature of $1200^{\circ}C{\sim}1400^{\circ}C$ for 10~60 minutes to enhance the color. All the seven specimen become darker and eventually be black as annealing temperature and time increase. The black samples turned into original colors when we elevated the temperature with oxy-acetylene torch for around 10 minutes in the air. Finally, we could tune the colors of cubic zirconia either anneal in vacuum or the black samples in the air to obtain the proposed colors. Our proposed new process may be appropriate to fabricate the precious synthetic colored cubic zirconia to simulate the natural colored gem quality diamonds.

스컬 용융법으로 제조된 유색 큐빅지르코니아의 색향상을 위해서 $1200^{\circ}C,\;1400^{\circ}C$에서 10~60분으로 조건을 바꾸면서 진공열처리를 실시하였다. 진공 열처리 시간과 온도가 증가함에 따라 준비된 7가지의 큐빅지르코니아는 점점 채도가 떨어지며 파스텔톤의 바디색을 유지하다가 궁극적으로 흑색으로 변화하였다. 흑색화가 완료된 시료는 다시 대기 중에서 산소토치를 이용하여 10분간 가열하면 원래의 색으로 환원되었다. 즉, 목표하는 색을 위해 진공 열처리를 진행하거나, 일단 진공열처리로 흑색화를 진행하고, 대기중 열처리를 통하여 목표하는 색을 가진 큐빅지르코니아의 색조정이 가능하였다. 이러한 신공정은 다이아몬드 보석재를 모사한 고부가가치 합성석으로 활용이 가능하였다.

Keywords

References

  1. N. Claussen, ""Fracture toughness of $Al_2O_3$ with an unstabilized $ZrO_2$ dispersed phase"", Journal of the American Ceramic Society, Vol. 59 (1-2), pp. 49-51, 1976. https://doi.org/10.1111/j.1151-2916.1976.tb09386.x
  2. F. F. Lange, "Transformation toughening - Part 4 Fabrication, fracture toughness and strength of Al2O3-ZrO2 composites", Journal of Materials Science, Vol. 17, pp. 247-254, 1982. https://doi.org/10.1007/BF00809060
  3. J. Wang, R. Stevens, "Toughening mechanisms in duplex alumina-zirconia ceramics", Journal of Materials Science, Vol. 23, No. 3, pp. 804-808, 1988. https://doi.org/10.1007/BF01153970
  4. M. Hirano, H. Inada, "Strength and phase stability of yttria-ceria-doped 정방정 zirconia /alumina composites sintered and hot isostatically pressed in argon-oxygen gas atmosphere", Journal of the American Ceramic Society, Vol. 74, pp. 606-611, 1991. https://doi.org/10.1111/j.1151-2916.1991.tb04067.x
  5. V. I. Aleksandrov, V. V. Osiko, A. M. Prokhrov, V. M. Tatarinntsev, "Synthesis and Crystal Growth of Refractory Materials by RF Melting in a Cold Container", North-Holland Publishing Co., Amsterdam, Netherlands, pp. 421-480, 1978.
  6. A. Baermann, W. Guse, H. Saalfeld, "Characterization of different (Me,Zr)O2 single crystals grown by the "skull-melting" technique", Journal of Crystal Growth, Vol. 79(1-3), pp. 331-335, 1986. https://doi.org/10.1016/0022-0248(86)90458-6
  7. D. B. Zhang, X. M. He, J. P. Chen, J. C. Wang, Y. F. Tang, B. L. Hu, "Research on crystal growth and defects in cubic zirconia", Vol. 79(1-3), pp. 336-340, 1986. https://doi.org/10.1016/0022-0248(86)90459-8
  8. R. C. Buchanan, S. Pope, "Optical and electrical propertees of yttria stabilized zirconia(YSZ) crystals". Journal of the Electrochemical Society, Vol. 130, No. 4, pp. 962-966, 1983. https://doi.org/10.1149/1.2119868
  9. K. R. Han, S. J. Park, K. S. Hong, H. W. Jun, "Preparation of Sintered ATZ by Sol-Gel Process and Properties", J. Kor. Soc. Anal. Sci., Vol. 6, No. 2, pp. 225-229, 1993.
  10. R. Aragon, "Skull melter single crystal growth of magnetite (Fe3O4)-ulvospinel (Fe2TiO4) solid solution members", Journal of Crystal Growth, Vol. 61, No. 2, pp. 221-228, 1983. https://doi.org/10.1016/0022-0248(83)90358-5
  11. D. Michel, M. Perez, Y. Jorba, R. Collongues, "Growth from skull-melting of zirconia-rare earth oxide crystals", Journal of Crystal Growth, Vol. 43, No. 4, pp. 546-548, 1978. https://doi.org/10.1016/0022-0248(78)90359-7
  12. 주기태 강봉훈, 적포도주색 큐빅상 지르코니아 단결정의 제조방법, 대한민국 특허등록번호 10-0768688-0000, 2007.
  13. 이재선, 녹색 큐빅지르코니아 단결정의 제조방법, 대한민국 특허등록번호 10-0509346-0000, 2005.
  14. 이재선, 청색 큐빅지르코니아 단결정의 제조방법, 대한민국 특허등록번호 10-0509345-0000, 2005.
  15. D.A. Proter and K.E. Eastering, "Phase tramsformation in metals and alloys", Van Nostrand Reinhold Co, Ltd, pp. 60-106, 1981.

Cited by

  1. Color Evolution in Single Crystal Colored Cubic Zirconias With Annealing Atmosphere and Temperature vol.53, pp.4, 2016, https://doi.org/10.4191/kcers.2016.53.4.450