Abstract
This paper presents the results of full-scale uplift load tests performed on 24 passive anchors grouted to various lengths at Okchun and Changnyong site. Rock anchors were installed over a wide range of rock types and qualities with a fixed anchored depth of 1~6 m. The majority of installations used D51 mm high grade steel rebar to induce rock failure prior to rod failure. However, a few installations included the use of D32 mm rebar at relatively deeper anchored depth so as to induce rod failure. In many tests, rock failure was reached and the ultimate loads were recorded along with observations of the shape and extent of the failure surface. In addition to field tests, laboratory pullout tests were conducted to determine bond strength and bond stress-shear slip relation at the tendon/grout interface when a corrosion protection sheath is installed in the cement-based grout. The test results show that the ultimate tendon-grout bond strength is measured from 18~25% of unconfined compressive strength of grout. One of the important results from these tests is that the measured strains along the corrosion protection sheath were so small that practically the reduction of bond strength by the presence of sheath would be negligible.
본 논문에서는 옥천 및 창녕지역에서 총 24회 수행한 암반앵커 현장인발시험의 결과를 나타내었다. 시험앵커의 정착깊이는 1~6m로 서로다른 암반내에 설치하였다. 앵커의 대부분은 고강도 이형철근인 SD40-D51mm를 사용함으로써 다른 파괴가 일어나기 전에 암반파괴가 먼저 일어나도록 유도하여 암반의 인발저항력을 파악하고자 하였으며, 일부에서는 SD40-D32mm앵커를 설치하여 앵커의 파괴도 아울러 살펴보았다. 많은 시험에서 파괴는 항복에 이르는 극한하중까지 관찰할 수 있었으며, 암반파괴형상은 암반이 들어올려지면서 방사상으로 균열이 발달하는 형태를 나타내었다. 또한 시멘트그라우트와 텐던사이의 부착강도를 평가하고자 방식쉬이스가 설치된 앵커에 대해 실내실험을 실시하였다. 실험결과 텐던-그라우트 사이의 부착강도는 그라우트 일축압축강도의 18~25%로 나타났으며, 방식쉬이스에 의한 부착력 감소는 무시할 수 있을 정도로 작게 나타났다.