DOI QR코드

DOI QR Code

The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramics

  • Kim, Hyung-Tae (Department of Prosthodontics, Graduate School, Seoul National University) ;
  • Han, Jung-Suk (Department of Prosthodontics, Graduate School, Seoul National University) ;
  • Yang, Jae-Ho (Department of Prosthodontics, Graduate School, Seoul National University) ;
  • Lee, Jai-Bong (Department of Prosthodontics, Graduate School, Seoul National University) ;
  • Kim, Sung-Hun (Department of Prosthodontics, Graduate School, Seoul National University)
  • Published : 2009.11.30

Abstract

STATEMENT OF PROBLEM. Recently Yttrium-stabilized tetragonal zirconia polycrystal (Y-TZP) has been introduced due to superior flexural strength and fracture toughness compared to other dental ceramic systems. Although zirconia has outstanding mechanical properties, the phenomenon of decrease in the life-time of zirconia resulted from degradation in flexural strength after low temperature aging has been reported. PURPOSE. The objective of this study was to investigate degradation of flexural strength of Y-TZP ceramics after various low temperature aging treatments and to evaluate the phase stability and micro-structural change after aging by using X-ray diffraction analysis and a scanning electron microscope (SEM). MATERIAL AND METHODS. Y-TZP blocks of Vita In-Ceram YZ (Vita Zahnfabrik, Bad $S\ddot{a}ckingen$, Germany) were prepared in 40 mm (length) $\times$ 4 mm (width) $\times$ 3 mm (height) samples. Specimens were artificially aged in distilled water by heat-treatment at a temperature of 75, 100, 125, 150, 175, 200, and $225^{\circ}C$ for 10 hours, in order to induce the phase transformation at the surface. To measure the mechanical property, the specimens were subjected to a four-point bending test using a universal testing machine (Instron model 3365; Instron, Canton, Mass, USA). In addition, X-ray diffraction analysis (DMAX 2500; Rigaku, Tokyo, Japan) and SEM (Hitachi s4700; Jeol Ltd, Tokyo, Japan) were performed to estimate the phase transformation. The statistical analysis was done using SAS 9.1.3 (SAS institute, USA). The flexural strength data of the experimental groups were analyzed by one-way analysis of variance and to detect statistically significant differences ($\alpha$= .05). RESULTS. The mean flexural strength of sintered Vita In-Ceram YZ without autoclaving was 798 MPa. When applied aging temperature at below $125^{\circ}C$ for 10 hours, the flexural strength of Vita In-Ceram YZ increased up to 1,161 MPa. However, at above $150^{\circ}C$, the flexural strength started to decrease. Although low temperature aging caused the tetragonal-to-monoclinic phase transformation related to temperature, the minimum flexural strength was above 700 MPa. CONCLUSION. The monoclinic phase started to appear after aging treatment above $100^{\circ}C$. With the higher aging temperature, the fraction of monoclinic phase increased. The ratio of monoclinic/tetragonal + monoclinic phase reached a plateau value, circa 75% above $175^{\circ}C$. The point of monoclinic concentration at which the flexural strength begins to decrease was between 12% and 54%.

Keywords

References

  1. Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 1999;15:426-33. https://doi.org/10.1016/S0109-5641(99)00070-6
  2. Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 1999;20:1-25. https://doi.org/10.1016/S0142-9612(98)00010-6
  3. Subbarao EC, Maiti HS, Srivastava KK. Martensitic transformation in zirconia. Phys Status Solidi Series A 1974;21:9-40. https://doi.org/10.1002/pssa.2210210102
  4. Kobayashi K, Kuwajima H, Masaki T. Phase change and mechanical properties of $ZrO_{2}-Y_{2}O_{3}$ solid electrolyte after ageing. Solid State Ionics 1981;3/4:489-93. https://doi.org/10.1016/0167-2738(81)90138-7
  5. Chevalier J, Cales B, Drouin JM. Low-temperature aging of Y-TZP ceramics. J Am Ceram Soc 1999;82:2150-204. https://doi.org/10.1111/j.1151-2916.1999.tb02055.x
  6. Lilley E. Review of low temperature degradation in Y-TZPs. In: Tressler RE, McNallan M, editors. Ceramic transaction: corrosion and corrosive degradation of ceramics. Westerville: American Ceramics Society, 1990:387-407.
  7. Lawson S. Environmental degradation of zirconia ceramics. J Eur Ceram Soc 1995;15:485-502. https://doi.org/10.1016/0955-2219(95)00035-S
  8. Deville S, Chevalier J, Fantozzi G, Bartolome JF, Requena J, Moya JS. Low-temperature ageing of zirconia-toughened alumina ceramics and its implication in biomedical implants. J Eur Ceram Soc 2003;23:2975-82. https://doi.org/10.1016/S0955-2219(03)00313-3
  9. Yoshimura M. Phase stability of zirconia. Am Ceram Sot Bull 1988;67:1950-5.
  10. Lube T, Manner M, Danzer R. The miniaturization of the 4-point bend test. Fatigue Fract. Engng Mater Struct 1997;20:1605-16. https://doi.org/10.1111/j.1460-2695.1997.tb01514.x
  11. Garvie RC, Nicholson PS. Phase analysis in zirconia systems. J Am Ceram Soc 1972;55:303-5. https://doi.org/10.1111/j.1151-2916.1972.tb11290.x
  12. Emsley J, The Elements (2nd ed.). Oxford University Press, Oxford, UK, 1991.
  13. Cales B, Stefani Y, Lilley E. Long-term in vivo and in vitro aging of a zirconia ceramic used in orthopaedy. J Biomed Mater Res 1994;28:619-24. https://doi.org/10.1002/jbm.820280512
  14. Shimizu K, Oka M, Kumar P, Kotoura Y, Yamamuro T, Makinouchi K, Nakamura T. Time-dependent changes in the mechanical properties of zirconia ceramic. J Biomed Mater Res 1993;27:729-34. https://doi.org/10.1002/jbm.820270605
  15. Pittayachawan P, McDonald A, Petrie A, Knowles JC. The biaxial flexural strength and fatigue property of Lava Y-TZP dental ceramic. Dent Mater 2007;23:1018-29. https://doi.org/10.1016/j.dental.2006.09.003
  16. Chevalier J, Deville S, Mu ¨nch E, Jullian R, Lair F. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis. Biomaterials 2004;25:5539-45. https://doi.org/10.1016/j.biomaterials.2004.01.002
  17. Cales B. Zirconia as a sliding material: histologic, laboratory, and clinical data. Clin Orthop Relat Res 2000;379:94-112. https://doi.org/10.1097/00003086-200010000-00013
  18. Deville S, Gremillard L, Chevalier J, Fantozzi G. A critical comparison of methods for the determination of the aging sensitivity in biomedical grade yttria-stabilized zirconia. J Biomed Mater Res B Appl Biomater 2005;72:239-45.
  19. Suarez MJ, Lozano JF, Paz Salido M, Martinez F. Three-year clinical evaluation of In-Ceram Zirconia posterior FPDs. Int J Prosthodont 2004;17:35-8.
  20. Oblak C, Jevnikar P, Kosmac T, Funduk N, Marion L. Fracture resistance and reliability of new zirconia posts. J Prosthet Dent 2004;91:342-8. https://doi.org/10.1016/j.prosdent.2004.01.009
  21. Roebben G, Basu B, Vleugels J, Van der Biest O. Transformationinduced damping behaviour of Y-TZP zirconia ceramics. J Eur Ceram Soc 2003;23:481-9. https://doi.org/10.1016/S0955-2219(02)00101-2
  22. Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 2005;33:9-18. https://doi.org/10.1016/j.jdent.2004.07.001
  23. Wen MY, Mueller HJ, Chai J, Wozniak WT. Comparative mechanical property characterization of 3 all-ceramic core materials. Int J Prosthodont 1999;12:534-41.
  24. Ardlin BI. Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure. Dent Mater 2002;18:590-5. https://doi.org/10.1016/S0109-5641(01)00095-1
  25. Aboushelib MN, de Jager N, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater 2005;21:984-91. https://doi.org/10.1016/j.dental.2005.03.013

Cited by

  1. Phase Stability and Mechanical Properties of Zirconia and Zirconia Composites vol.10, pp.1, 2013, https://doi.org/10.1111/j.1744-7402.2011.02717.x
  2. Effects of a convenient silica-coating treatment on shear bond strengths of porcelain veneers on zirconia-based ceramics vol.31, pp.5, 2012, https://doi.org/10.4012/dmj.2012-037
  3. Raman Spectroscopy Evaluation of Subsurface Hydrothermal Degradation of Zirconia vol.95, pp.7, 2012, https://doi.org/10.1111/j.1551-2916.2012.05237.x
  4. Low-temperature degradation of a Y-TZP ceramic after surface treatments vol.101, pp.8, 2013, https://doi.org/10.1002/jbm.b.32957
  5. Two-body wear of monolithic, veneered and glazed zirconia and their corresponding enamel antagonists vol.71, pp.1, 2013, https://doi.org/10.3109/00016357.2011.654248
  6. Zirconia Implants with Laser Surface Treatment: Peri-Implant Bone Response and Enhancement of Osseointegration vol.23, pp.1, 2014, https://doi.org/10.2485/jhtb.23.93
  7. Influence of Implant Angulation on the Fracture Resistance of Zirconia Abutments vol.24, pp.2, 2014, https://doi.org/10.1111/jopr.12182
  8. Monoclinic phase transformation and mechanical durability of zirconia ceramic after fatigue and autoclave aging vol.105, pp.7, 2017, https://doi.org/10.1002/jbm.b.33720
  9. Surface and Mechanical Characterization of Dental Yttria-Stabilized Tetragonal Zirconia Polycrystals (3Y-TZP) After Different Aging Processes vol.22, pp.06, 2016, https://doi.org/10.1017/S1431927616011843
  10. Influence of Accelerated Aging on the Color Stability of Dental Zirconia vol.28, pp.5, 2016, https://doi.org/10.1111/jerd.12239
  11. Effect of different grinding burs on the physical properties of zirconia vol.8, pp.2, 2016, https://doi.org/10.4047/jap.2016.8.2.137
  12. Influence of Different Framework Designs on the Fracture Properties of Ceria-Stabilized Tetragonal Zirconia/Alumina-Based All-Ceramic Crowns vol.9, pp.5, 2016, https://doi.org/10.3390/ma9050339
  13. Fatigue behaviours of the zirconia dental restorations prepared by two manufacturing methods vol.116, pp.7, 2017, https://doi.org/10.1080/17436753.2017.1336365
  14. Fracture resistance of zirconia-composite veneered crowns in comparison with zirconia-porcelain crowns vol.36, pp.3, 2017, https://doi.org/10.4012/dmj.2016-298
  15. Grinding With Diamond Burs and Hydrothermal Aging of a Y-TZP Material: Effect on the Material Surface Characteristics and Bacterial Adhesion vol.42, pp.6, 2017, https://doi.org/10.2341/16-108-L
  16. Effects of Silica Coating by Physical Vapor Deposition and Repeated Firing on the Low-Temperature Degradation and Flexural Strength of a Zirconia Ceramic pp.1059941X, 2017, https://doi.org/10.1111/jopr.12618
  17. Shear Bond Strengths between Three Different Yttria-Stabilized Zirconia Dental Materials and Veneering Ceramic and Their Susceptibility to Autoclave Induced Low-Temperature Degradation vol.2016, pp.None, 2009, https://doi.org/10.1155/2016/9658689
  18. Fracture Load and Phase Transformation of Monolithic Zirconia Crowns Submitted to Different Aging Protocols vol.41, pp.5, 2016, https://doi.org/10.2341/15-154-l
  19. Effects of multiple firings on the low-temperature degradation of dental yttria-stabilized tetragonal zirconia vol.115, pp.4, 2009, https://doi.org/10.1016/j.prosdent.2015.08.029
  20. Effect of Different Coloring Procedures on the Aging Behavior of Dental Monolithic Zirconia vol.2018, pp.None, 2009, https://doi.org/10.1155/2018/2137091
  21. Effect of grinding and aging on subcritical crack growth of a Y-TZP ceramic vol.32, pp.None, 2009, https://doi.org/10.1590/1807-3107bor-2018.vol32.0032
  22. Influence of Solid Loading on the Granulation of 3Y-TZP Powder by Two-Fluid Spray Drying vol.55, pp.4, 2009, https://doi.org/10.4191/kcers.2018.55.4.04
  23. Y-TZP surface behavior under two different milling systems and three different accelerated aging protocols vol.67, pp.6, 2009, https://doi.org/10.23736/s0026-4970.18.04138-9
  24. Fracture Toughness of 3Y-TZP Dental Ceramics by Using Vickers Indentation Fracture and SELNB Methods vol.56, pp.1, 2019, https://doi.org/10.4191/kcers.2019.56.1.01
  25. Effect of surface treatments and aging on phase transformation and flexural strength of different Y‐TZP ceramics vol.16, pp.4, 2019, https://doi.org/10.1111/ijac.13238
  26. Optical and mechanical properties of purple zirconia ceramics vol.7, pp.3, 2009, https://doi.org/10.1080/21870764.2019.1629862
  27. Ageing assessment of zirconia implant prostheses by three different quantitative assessment techniques vol.11, pp.5, 2019, https://doi.org/10.4047/jap.2019.11.5.253
  28. Fracture Resistance of Zirconia Oral Implants In Vitro: A Systematic Review and Meta-Analysis vol.13, pp.3, 2009, https://doi.org/10.3390/ma13030562
  29. Effect of ionizing radiation on mechanical properties and translucency of monolithic zirconia vol.108, pp.3, 2020, https://doi.org/10.1002/jbm.b.34458
  30. Impact of multiple firings and resin cement type on shear bond strength between zirconia and resin cements vol.12, pp.4, 2009, https://doi.org/10.4047/jap.2020.12.4.197
  31. Effects of low-temperature degradation on the surface roughness of yttria-stabilized tetragonal zirconia polycrystal ceramics: A systematic review and meta-analysis vol.125, pp.2, 2009, https://doi.org/10.1016/j.prosdent.2020.01.005
  32. Effect of air‐abrasion at pre‐ and/or post‐sintered stage and hydrothermal aging on surface roughness, phase transformation, and flexural strength of multilayered monolithic zirco vol.109, pp.4, 2009, https://doi.org/10.1002/jbm.b.34760
  33. Effects of surface roughness of ceria-stabilized zirconia/alumina nanocomposite on the morphology and function of human gingival fibroblasts vol.40, pp.2, 2021, https://doi.org/10.4012/dmj.2019-435
  34. Influence of Preaging Temperature on the Indentation Strength of 3Y-TZP Aged in Ambient Atmosphere vol.14, pp.11, 2009, https://doi.org/10.3390/ma14112767
  35. Intraoral low-temperature degradation of monolithic zirconia dental prostheses: Results of a prospective clinical study with ex vivo monitoring vol.37, pp.7, 2009, https://doi.org/10.1016/j.dental.2021.03.008
  36. Surface and bulk properties of zirconia as a function of composition and aging vol.126, pp.None, 2009, https://doi.org/10.1016/j.jmbbm.2021.104994