SEM/EDS Evaluation of Gold Bonding Agent Applied on Non-precious Alloys and Cast CP-Ti

도재 소부용 비귀금속 합금과 티타늄에 적용한 Gold Bonding Agent의 전자현미경적 평가

  • Lee, Jung-Hwan (Department of Denial Laboratory Technology, Gwang-Ju Health college University) ;
  • Ahn, Jae-Seok (Denial Laboratory, Korea University Ansan Hospital)
  • 이정환 (광주보건대학 치기공과) ;
  • 안재석 (고려대학교의료원 안산병원 치과기공실)
  • Received : 2009.04.07
  • Accepted : 2009.06.05
  • Published : 2009.06.30

Abstract

The purposed of this study was to investigate the effect of Gold bonding agent as intermediate layer between metal substrate and ceramic coating. Gold bonding agent used to seal off any surface porosity, to mask the greyish color of the metal, and to provide an underlying bright golden hue to the ceramic coverage. The adhesion between metal substrate and ceramic is related to diffusion of oxygen during ceramic firing. The oxide layer produced on non-precious alloy anti titanium was considered to have a potentially adverse effect on metal-ceramic bonding. The oxidation characteristics of titanium and non-precious alloys are the main problem. Every group were divided into test and control groups. Control groups are carried out process of degassing for product oxide layer. Au coating was applied on each Ni-Cr, Co-Cr alloys and cp-Ti specimens with difference surface condition or degassing. Specimens surfaces and cutting plane was characterized by SEM/EDS. Results suggested that Au coating is effective barriers to protect metal oxidation during ceramic firing.

본 연구는 금속-도재 수복물 제작에 사용되는 Ni-Cr alloy와 Co-Cr alloy, 그리고 티타늄에 gold bonding agent를 도포하여 Au coating 층을 형성하였다. 각 시편의 절단면을 전자현미경으로 Au coating 층과 porcelain bonder, 그리고 불투명 도재간의 결합을 관찰하였고, 각 계면의 상태를 SEM/EDS 방법으로 조사하였다. 실험에서 사용된 재료와 방법의 범위 내에서 다음과 같은 결론을 얻었다. 1. Gold bonding agent를 사용하여 형성한 Au coating 층은 미세다공성을 가진 구조로 판단되었다. 2. Au coating 층과 porcelain bonder 그리고 불투명 도재간의 결합은 잘 일어나 보였다. 3. Au coating 층은 도재 소성과정에서 발생하는 산화층의 확산을 제한하는 것으로 관찰되었다.

Keywords

References

  1. Shell JS, Nielsen JP: Study of the bond between gold alloys and porcelain. J Dent Res 41: 1424-1437, 1962. https://doi.org/10.1177/00220345620410062101
  2. Baran, GR: Oxidation kinetics of some Ni-Cr alloys. J. Dent. Res 62: 51-55, 1983. https://doi.org/10.1177/00220345830620011101
  3. Baran, GR: Auger chemical analysis of oxides on Ni-Cr alloys. J Dent Res 63: 76-80, 1984. https://doi.org/10.1177/00220345840630012001
  4. Adachi M, Mackert JR, Parry EE, Fairhurst CW: Oxide adherence and porcelain bonding to titanium and Ti-6AI-4V alloy. J Dent Res 69: 1230-1235, 1990. https://doi.org/10.1177/00220345900690060101
  5. Taira Y, Yanagida H, Matsumura H, Yoshida K, Atsuta M, Suzuki S: Adhesive bonding of titanium with a thionephosphate dual functional primer und self-curing luting agents. Eur J oral Sci 108: 456-460, 2000. https://doi.org/10.1034/j.1600-0722.2000.108005456.x
  6. Low D, Sumii T, Swain M: Thermal expansion coefficient of titanium casting. J Oral Rehabil 28: 239-242, 2001.
  7. Cecconi BT, Koeppen RG, Phoenix RD, Cecconi ML: Casting titanium partial denture frameworks: a radiographic evaluation. J Prosthet Dent 87: 277-280, 2002. https://doi.org/10.1067/mpr.2002.122275
  8. Park SY, Jeon YC, Jeong CM: Comparison of the bond strength of ceramics fused to titanium and Ni-Cr alloy. J Korean Acad Prosthodont 41(1): 89-98, 2003.
  9. Cai Z, Bunce N, Nunn ME, Okabe T: Porcelain adherence to dental cast CP titanium: effects of surface modifications. Biomaterials 22(9): 979-986. 2001. https://doi.org/10.1016/S0142-9612(00)00263-5
  10. McLean JW: The Metal-ceramic restoration. Dent Clin North Am 27:747-761, 1983.
  11. Moffa JP, Lugassy AA, Guckes AD, Gottleman L: An evaluation of nonprecious alloys for use with porcelain veneers, Pan l: Physical properties. J Prosthet Dent 30: 424-431, 1973. https://doi.org/10.1016/0022-3913(73)90164-9
  12. Ozcan I. Uysal H: Effects of silicon coating on bond strength of two different titanium ceramic to titanium. Dental Materials 21: 773-779, 2005. https://doi.org/10.1016/j.dental.2005.01.014
  13. Russell RW, Gerhard EW, Othon Monteiro: Silicon nitride coating on titanium to enable titanium-ceramic bonding. J Biomed Mater Res 46: 262-270, 1999. https://doi.org/10.1002/(SICI)1097-4636(199908)46:2<262::AID-JBM16>3.0.CO;2-1
  14. Russell RW. Kon KF: Oxidation behavior of surface-modified titanium for titanium-ceramic restorations. J Prosthet Dent 77: 423-434, 1997. https://doi.org/10.1016/S0022-3913(97)70168-9
  15. Lee KM, Cai Z, Griggs JA, Guiatas L, Lee DJ, Okabe T: SEM/EDS evaluation of porcelain adherence to gold-coated cast titanium. J Biomed Mater Res PartB: Appl Biomater 68B: 165-173, 2004. https://doi.org/10.1002/jbm.b.20017
  16. HerH, Austrheim E: Gold-based bonding agents between palladium-alloys and ceramic veneer. Dent Mater 3: 168-175, 1987. https://doi.org/10.1016/S0109-5641(87)80029-5
  17. Goeller I. Meyer JM. Nally JN: Comparative study of three coating agents and their influence on bond strength of porcelain-fused-to-gold alloys. J. Prosthet Dent 28: 504-511, 1972. https://doi.org/10.1016/0022-3913(72)90062-5
  18. Ciftci Y, Canay S, Hersek N: Shear bond strength evaluation of different veneering systems on Ni-Cr alloys. J Prosthodont 16:31-36, 2007. https://doi.org/10.1111/j.1532-849X.2006.00148.x
  19. Saadet A, Semih B: Bond strength of three porcelains to two forms of titanium using two firing atmosphere. J Prosthet Dent 84: 567-574, 2000. https://doi.org/10.1067/mpr.2000.110267
  20. Prbster L, Maiwald U, Weber H: Threepoinr bending strength of ceramics fused to cast titanium. Eur J Oral Sci 104: 313-319, 1996. https://doi.org/10.1111/j.1600-0722.1996.tb00083.x
  21. Kimura H, Horng CJ, Okazaki M, Takahashi J: Effects of retention and bonding agent on bond strength of the titanium-porcelain system. J Osaka Uni Dent Sch 31: 23-32, 1991.
  22. Robert J. Dent, Jack D. Preston, Joseph P. Moffa, Angelo Caputo: Effect of oxidation on ceramometal bond strength. J Prosthet Dent 47: 59-62, 1982. https://doi.org/10.1016/0022-3913(82)90243-8
  23. Papazoglou E, William A. Brantley William M. Johnston, Alan B. Carr: Effects or dental laboratory processing variables and in vitro testing medium on the porcelain adherence of high-palladium casting alloys. J Prosthet Dent 79: 514-519, 1998. https://doi.org/10.1016/S0022-3913(98)70171-4
  24. Thomas A. Wight, John C. Bauman, George B. Pelleu Jr: An evaluation of four variables affecting the bond strength of porcelain to nonprecious alloy. J Prosthet Dent 37: 570-577, 1977. https://doi.org/10.1016/0022-3913(77)90172-X