초록
The aim of this study is to investigate the full annealing parameter for A3003 Al alloy welded tubes. The A3003 Al alloy tubes with 34 mm in external diameter and 1.3 mm in thickness for OPC drum were manufactured by high frequency induction welding with the V shaped convergence angle $6.7^{\circ}$ and power input 50 kW. The tensile and yield strength decreased with increasing the annealing temperature and time remarkably, but elongation increased remarkably. Vickers hardness in welds and base metal decreased with increasing the annealing temperature and time remarkably. In a certain experimental condition, the welds line in A3003 alloys disappeared at $520^{\circ}C$ for 4hr because of the same mechanical properties and structures between welds and base metal.