Effect of Si/$Si_3N_4$ Ration on the Micro structure and Properties of Porous Silicon Nitride Prepared by SHS Method

규소/질화규소 비가 자전연소합성공정을 이용한 다공질 질화규소 세라믹스의 미세구조와 특성에 미치는 영향

  • 김동백 (창원대학교 재료공학부) ;
  • 박동수 (한국기계연구원 재료연구부) ;
  • 한병동 (한국기계연구원 재료연구부) ;
  • 정연길 (창원대학교 재료공학부)
  • Published : 2004.12.30

Abstract

Porous silicon nitride ceramics were prepared by Self-propagating High Temperature Synthesis from silicon powder, silicon nitride powder and the pore-forming precursor. The microstructure, porosity and the flexural strength of the porous silicon nitride ceramics were varied according to the Si/$Si_3N_4$ ratio, size and amount of the pore-forming precursors. Some samples exhibited as high flexural strength as $162\pm24$ MPa. The high strength is considered to result from the fine pore size and the strong bonding among the silicon nitrid particles.