Abstract

Generally, reinforced concrete is one of the most commonly used structural materials and it prevents corrosion of steel bar by high pH of interior, But, as time elapsed, reinforced concrete structure become deteriorated by many of combined deterioration factors and environmental conditions. And, there are large number of deteriorate mechanism of the reinforced concrete structure and it acts complexly. It is recognized that steel bar corrosion is the main distress behind the present concern regarding concrete durability. In this study, to institute combined deterioration environments, established acceleration condition and cycle for combined deterioration environments has a resemblance to environments which are real structures placed. After that to confirm corrosion properties of reinforced concrete due to permeability with covering depth and types of surface cover under combined deterioration environments, measured carbonation velocity coefficients, chloride ion diffusion coefficients, water absorption coefficients, air permeability coefficients and electric potential, corrosion area ratio, weight reduction, corrosion velocity of steel bar. The results showed that an increase in age also decrease carbonation velocity coefficients, increase Chloride ion diffusion coefficients and increases water absorption coefficients. As well, an increase in age also increases corrosion of steel bar. Data on the development of corrosion velocity of steel bar with types of surface cover made with none, organic B, organic A, inorganic B, and inorganic A is shown. As well, permeability and corrosion velocity of steel bar with covering depth is superior to 10mm than 20mm. And it is confirmed permeability and corrosion properties of steel bar are closely related.

Keywords

References

  1. 金武漢 ほか,コンクリートの急速鹽分浸透性試驗による鹽化物イオン擴散係數の評價に關する實的硏究, 日本建築學會 學術講演梗槪集, 2003, pp.561-562.
  2. 김무한 외, 마감재종류에 따른 염소이온 확산특성에 관한 실험적 연구, 한국콘크리트학회 가을 학술발표대회 논문집, 2002. pp.327-331.
  3. 渡辺 豊 ほか,コンクリ一の急速鹽分浸透性試驗による鹽化物イオン壙散係數の算定, コンクリ一ト工學年次論文集, 2002. pp.663-668.
  4. 日本コンクリ一ト工學協會, 複合劣化コンクリ一ト構造物の 評價と 維持管理計劃硏究委員會, 2001,5
  5. R.D. Browne, Mechanism of Corrosion of Steel in Relation to Design, Inspection, and Repair of Offshore and Coastal Structure, ACI SP-65, U.S. Detroit, 1980
  6. Tang, I. and Nilsson, L.-O.,Rapid Determination of the Chlolide Diffusivity in Concrete by Applying an Electrical Field, ACI Materials Journal, Jan.-Feb. 1992, pp.49-53.
  7. R.D. Browne, Mechanism of Corrosion of Steel in Relation to Design, Inspection, and Repair of Offshore and Coastal Structure, ACI SP-65, U.S. Detroit, 1980
  8. Page, C.L., Diffusion of Chloride Ions in Hardened Cement Pastes, Cement and Concrete Reseach, 11, 1981, 395-406 https://doi.org/10.1016/0008-8846(81)90111-3