초록

The sliding wear characteristics of the crane sheave were investigated using a pin-on-disk rig tester. The experiment was conducted using a high carbon steel wire that was upper material, also carbon steel castings that was disk material. There are various operating conditions in this work. At the room temperature, we carried out the wear test under a grease lubrication and dry condition. The results of wear test showed that an annealed-casted have lower, also the wear curves are linearly increased with increasing of sliding distance. For the specific wear rate of annealed-casted, the wear resistance was increased with decreasing diameter of wire. The wear of a wire and a disk have a different mechanism, the one is the abrasive wear due to fatigue wear under lubrication, another is the adhesion wear under dry condition.

키워드

참고문헌

  1. Cranes-Design, Practice, Maintenance J.Verschoof
  2. KS B 0127, 한국공업규격 크레인 용어(종류)
  3. KS B 4731, 한국공업규격 시브
  4. Injury Cultent Situation Ministy of Labor Republic of Korea
  5. KS D 3514, 한국공업규격 와이어-로프
  6. Wire-Rope Users Manual(Second edition) American Iron and Steel Institute
  7. KS D 4101, 한국공업규격 탄소주강품
  8. KS D 3559, 한국공업규격 경강선재
  9. 기계재료 한현수;박인홍;김정배
  10. 대한기계학회논문집 v.20 no.5 탄소강의 가공조건과 마찰·마멸과의 관계 정종현;김대은
  11. 대한기계학회논문집 v.26 no.4 잔류응력의 표면 파손과 마멸에 대한 영향 김진욱;이영제
  12. CIRP v.36 Residual Stresses as Essential Criteria for the Evaluation of Production Processes Leskovar,I.P;Ferlan,M.Sc.D.;Kovac,I.M. https://doi.org/10.1016/S0007-8506(07)62633-X
  13. Wear v.65 Application of the oxidational theory of mild wear to the sliding wear of low alloy steel T.F.J.Quinn;D.M.Rowson;J.L.Sullivan https://doi.org/10.1016/0043-1648(80)90002-2
  14. Wear v.121 A study of mild oxidational wear for conditions of low load and speed J.L.Sullivan;S.G.Hodgson https://doi.org/10.1016/0043-1648(88)90033-6
  15. Wear v.95 On the critical thickness of protective films at sliding interfaces R.Y.Lee;Z.Eliezer https://doi.org/10.1016/0043-1648(84)90115-7
  16. proceedings of the JSLE-ASLE International lubrication conference Effect of cold-working and grain size on wear of steel Endo,K.;Okada,T.;Iwai,Y.
  17. Engineering Failure Analysis v.8 Effect of degradation and impaired quality on wire rope bending of sheave fatigue endurance I.M.L.Ridge;C.R.Chaplin;J.Zheng https://doi.org/10.1016/S1350-6307(99)00051-5
  18. Journal of Testing and Evaluation, JTEVA v.22 no.5 Wear-related fatigue in a wire-rope failure Schrems,K.K. https://doi.org/10.1520/JTE12670J