A Study on the Mix Design of Antiwashout Underwater Concrete According to Compressive Strength

압축강도에 따른 수중불분리 콘크리트의 배합설계에 관한 연구

  • Published : 2003.09.01

Abstract

At present, the antiwashout underwater concretes are used as popular construction materials in European countries, the United States and Japan. The water-soluble polymers in the antiwashout underwater concretes provide excellent segregation or washout resistance, self-compaction and self-leveling property to the concretes. The purpose of this study is to recommend to optimum mix proportions of antiwashout underwater concretes according to compressive strength of 300kgf/$\textrm{cm}^2$ to 500kgf/$\textrm{cm}^2$. The antiwashout underwater concretes are prepared with various unit cement content, unit water content, sand-aggregate ratio, unit antiwashout agent and superplasticizer content. And they are tested for flowability, and compressive strength. From the test results, it is possible to recommend the optimum mix proportions of antiwashout underwater concretes according to compressive strengths within the range of 300kgf/$\textrm{cm}^2$ to 500kgf/$\textrm{cm}^2$.

Keywords

References

  1. 山口ほか ; 水中コンクリ一ト(ケイクリ一ト)の開發とぞの適用, '橋梁' Vol.21, No.2, 1985.
  2. 芳賀ほか ; 分離低減劑を用いた水中コンクリ一トに關する硏究, '第6回コンクリ一ト工學年次講演會論文集, 1984
  3. K.H.khayat, Effects of Antiwashout Admixtures on Fresh Concrete Properties, ACI Structural Journal, March-April. pp.164-170, 1995
  4. 오상근, 조인성, 수중불분리 혼화제, 한국콘크리트학회지, 제8권 2호, pp.41-48, 1996
  5. 이병덕 외 2인, 양생온도에 따른 수중불분리성 콘크리트의 물리.역학적특성, 한국콘크리트학회 1997년 봄 학술발표대회 논문집, pp.301-307, 1997. 3.