A Study on High Temperature Particles-Erosion of Hard Coatings

경질 코팅의 고온 입자침식 현상 연구

  • 이의열 (안동대학교 신소재공학부 금속재료) ;
  • 김종하 (안동대학교 신소재공학부 금속재료)
  • Published : 2003.08.01

Abstract

Many steam turbine components encounter solid particle erosion damage. It has been reported that particle erosion damage is caused by oxide scale exfoliation from boiler tubes. One of the most effective solutions to combat the erosion damage is the application of erosion resistant coatings on the turbine components. In this study, particle erosion resistance for various hard coatings such as nitride, Cr carbide and boride coatings was evaluated under the simulated erosion conditions of steam turbines. Based on the particle erosion tests, the boride coating was found to be more superior to others.

Keywords

References

  1. W. Tabakoff, M. Metwally, A. Hamed, Transactions of the ASME, 117 (1995) 146-148 https://doi.org/10.1115/1.2822295
  2. B. Formanek, Materials Science Forum, 163 (1994)317-322 https://doi.org/10.4028/www.scientific.net/MSF.163-165.317
  3. Chatterjee-Fischer. R, and Schaaber. O, Proceedings of Heat Treatment, Stratford-upon-Avon, Metals Society (1976) 27-30
  4. K. C. Goretta and A. C. Thompson, Materials Science and Engineering, 56 (1993) 7-10
  5. A. V. Levy, Surface and Coatings Technology, 36( 1988) 387-406 https://doi.org/10.1016/0257-8972(88)90168-5
  6. M. Jiang, K. C. goretta, EPRI Journal (1990) 30-37
  7. A. V. Levy, J. Yan and J. Patterson, Wear, 108 (1986) 61-76 https://doi.org/10.1016/0043-1648(86)90088-8
  8. B. Venkataraman, G. Sundarajan, Surface and Coatings Technology, 73 (1995) 177-184 https://doi.org/10.1016/0257-8972(94)02379-4
  9. B. Venkataraman, G. Sundarajan, Surface and Coatings Technology, 73 (1995) 177-184 https://doi.org/10.1016/0257-8972(94)02379-4