초록
The homogeneous distribution of solid region without liquid segregation is important in terms of high quality component during thixoforming process. In closed die semi-solid forging process, liquid segregation is strongly affected by injection velocity than solid fraction because the material has to travel relatively long distance to fill the cavity through a narrow gate. The designed die by computer simulation data was used to thixoforging process. The thixoforming velocity to prediction the liquid segregation had been determined with strain rate associated with multistage velocity control during compression test of semi-solid material. The optimal forging velocity and die temperature were investigated to produce the near-net-shape compressor component. The mechanical properties of thixoformed component were tested with various die and material temperatures before and after heat treatment.