Characterization of Hydrothermally Synthesized $BaTiO_3$ Powder and Spark Plasma Sintering(SPS)

수열합성 법에 의한 $BaTiO_3$ 분말제조 및 방전 플라즈마 소결

  • 이정수 (한양대학교 금속재료공학과) ;
  • 이완재 (한양대학교 금속재료공학과)
  • Published : 2001.03.01

Abstract

$BaTiO_3$ fine powder was synthesized by hydrothermal process from the mixture of titania-hydroxide($TiO_2{\cdot}xH_2O$) and barium hexa-hydroxide ($Ba(OH)_2{\cdot}8H_2O$) as starting materials. Fine powder(< 100 nm) was made under the reaction conditions of 18$0^{\circ}C$,10 atm, 1.5 hr in autoclave and showed cubic structure. The powders were sintered by a spark plasma sintering technique from 1050~115$0^{\circ}C$ for 5 min. The grains of sample sintered at 110$0^{\circ}C$ were about 0.9${\mu}m$ in average size and showed the mixture of cubic and tetragonal structures.

Keywords

References

  1. J. Mater. Sci. v.30 B.Huybrechts;K.Ishizaki;Takata
  2. J. Appl. Phys. v.66 D.C.Sinclair;A.R.West
  3. Electroceramics A.J.Moulson;J.M.Herbert
  4. J. Am. Ceram. Soc. v.68 Y.Ohara;K.Koumoto;H.Yanagida
  5. IEEE J. Quantum Electron. v.23 R.S.Hathcock;D.A.Temple;C.Warde
  6. Jpn. J. Appl. Phys. v.35 H.Kanai;K.Handa;Y.Yamashita;K.Hasegawa;S.Mukaeda;K.Handa
  7. J. Mater. Sci. v.25 P.P.Phule;S.H.Risbud
  8. Sol-gel Technology for Thin Films, Fibers, Preforms, Electronics and Specialty Shapes L.C.Klein
  9. J. European Ceram. Soc. v.20 S.Suasmoro;S.Pratapa;D.Setyoko;U.M.Dani
  10. J. Mater. Res. v.11 L.Zhao;A.T.Chien;F.F.Lange;J.S.Speck
  11. Jpn. J. Appl. Phys. v.36 W.Zhu;S.A.Akbar;R.Asiaiel;P.K.Dutta
  12. J. European Ceram. Soc. v.20 M.Viviani;J.Lemaitre;M.T.Buscaglia;P.Nanni
  13. J. Mater. Sci. v.34 T.Takeuchi;E.Betourne;M.Tabuchi;H.Kaneyama;Y.Kobayashi;A.Coats;F.Morrison;D.C.Sinclair;A.R.West.
  14. J. Am. Ceram. Soc. v.72 K.Uchino;E.Sadanaga;T.Hirose
  15. J. Am. Ceram. Soc. v.22 R.Virekanandan;S.Philip;T.R.N.Kutty
  16. Mater, Lett. v.5 T.R.N.Kutty;R.Virekanadan