Fretting Wear Mechanisms of TiN Coated Nuclear Fuel Rod Cladding Tube

TiN 코팅한 핵연료봉 피복재의 프레팅 마멸기구

  • 김태형 (경북대학교 기계공학과 대학원) ;
  • 성지현 (경북대학교 기계공학과 대학원) ;
  • 김석삼 (경북대학교 기계공학부)
  • Published : 2001.12.01

Abstract

The fretting wear of a nuclear fuel rod it a dangerous phenomenon. In this study, TiN coating was used to reduce the fretting wear of Zircaloy-4 tube, a nuclear fuel rod cladding material. TiN coating is probably one of the molt frequently and successfully used PVD coatings for the mitigation of fretting wear. The fretting tester was designed and manufactured for this experiment. The number of cycles, slip amplitude and normal load were selected as main factors of fretting wear. The results of this research showed that wear volume was improved 1.3∼3.2 times with TiN coating. The worn surfaces were observed by SEM. Wear mechanism at lower slip amplitude was the brittle cracks and rupture of TiN coating. However, adhesive and abrasive wear were mainly observed on most surfaces at higher slip amplitude.

Keywords

References

  1. 한국전력공사 홈페이지 한국전력공사
  2. 산업정보망 에너지 연별 통계
  3. KNFC KEPCO Nuclear Co.
  4. IAEA Press Releases v.25 IAEA Press
  5. Glossary of Terms and Definitions in the Field of Friction, Wear and Lubrication (Tribology) OECD
  6. Recent trend in studies of fretting wear, Trans. v.30 Sato, J.
  7. Wear v.153 Mechanics and Materials in Fretting Vincent, L.;Berthier, Y.;Dubourg, M. C.;Godet, M.
  8. ASTM STP144 Campbell, W.E.
  9. Journal of Materials Processing Technology v.99 Some considerations on the mitigation of fretting damage by the application of surface- modification technologies Fu, Y.;Wei, J.;Batchelor, A. W.
  10. Wear v.210 On the behavior of an oil lubricated fretting contact Shima, M.;Suetake, H.;McColl, I. R.;Waterhouse R. B.;Takeuchi, M.
  11. Wear v.225-229 Ni-P and Mo : an excellent fretting wear resistant combination Okado, J.;Shima, M.;McColl, I. R.;Waterhouse, R. B.;Hasegawa, T.;Kasaya, M.
  12. Wear v.224 A comparative study on fretting wear-resistant properties of ion-plated TiN and magnetron-sputtered MoS₂ coatings Xu, G. Z.;Zhou, Z. R.;Liu, J. J.
  13. Wear v.181-183 Fretting of Titanium nitride and diamond like carbon coatings at high frequencies and low amplitude Schouterder, K.;Blanpain, B.;Celis, J. P.;Vinsbo, O.
  14. Surf Coat. Technol. v.74-75 Hard coatings under vibration contact conditions Blanpain, B.;Mohrbacher, H.;Liu, E.;Celis, J. P.;Ross, J. R.
  15. Proc. Roy. Soc. Lond. Ser. A v.236 The fretting corrosion of mild steel Hallyday, J. S.;Hirst, W.
  16. The Effect of Slip Amplitude and Load in Fretting Wear v.44 no.378 Iwabuchi, A.
  17. Proc. Instn. Mech. Engrs v.197C Explicit equations for the stresses beneath a sliding spherical contact Hamilton, G. M.