Abstract
$(Ba_{0.6}Sr_{0.4}Ca_x)TiO_3 + yAl_2O_3$ wt% (x=0.10, 0.15, 0.20, y=0~3.0) ceramics were fabricated by the mixed-oxide method, and their structural and dielectric properties were investigated with variation of composition ratio and $Al_2O_3$ doping content. As results of the X-ray diffraction and microstructure analysis, all BSCT specimens showed dense and homogeneous structure without presence of the second phase. The sintered density was decreased with an increase of $Al_2O_3$ doping content. The Curie temperature and relative dielectric constant at room temperature were decreased with increasing $Al_2O_3$doping content. The dielectric loss is minimum at BSCT doped with 1.5wt% $Al_2O_3$content. The tunability was decreased with increasing an Ca content and the BSCT(50/40/10) specimen doped with 2.0wt% $Al_2O_3$content showed the maximum value of 4.2%.