Acknowledgement
Supported by : 조선대학교
In this study, adaptation of compomer to saliva contaminated dentin was evaluated with scanning electron microscope(SEM) and confocal laser scanning microscope(CLSM). For the SEM study, the occulusal surfaces of thirty two molar teeth were grounded to exposure dentin surfaces. The specimen were randomly assigned to control and three experimental groups with four samples in each group. In control group, Dyract and F-2000 compomer were bonded on the specimens according to the manufactures direction. Experimental groups were subdivided into three groups. They were contaminated with saliva on dentin surfaces ; Experimental group 1 : Saliva was dried with compressed air. Experimental group 2 : Saliva was rinsed with air-water spray and dried. Experimental group 3 : After polymerization of an adhesive, they were contaminated with saliva, and then saliva was rinsed with air-water spray and dried. Dyract and F-2000 compomer were bonded on saliva-treated dentin surfaces. The interfaces between dentin and compomer were observed with SEM. For the CLSM study, Class V cavities were prepared in buccal and ligual surfacess of thirty two molars. The specimens were divided into control and experimental groups. Class V cavities in experimental group were contaminated with saliva and those surfaces in each experimental groups received the same treatments as for the SEM study. Cavities were applied Prime & Bond 2.1 and F-2000 compomer primer/adhesive that were mixed with fluorescein, and then were filled with Dyract and F-2000 compomer. Specimens were embedded in transparent acrylic resin and sectioned buccolingual1y with diamond wheel saw, and then mounted on cover slide for CLSM study. The interface between cavity and compomer was observed by fluoresence imaging with a CLSM. The results were as follows : 1. In SEM exammination of Dyract group, control group, experimental group 2, 3 showed close adaptation to dentin and hybrid layer of
Supported by : 조선대학교