SHEAR BOND STRENGTH OF DENTIN BONDING AGENTS ON DENTIN SURFACE TREATED WITH EUGENOL

유지놀 처리된 상아질 표면의 상아질 접착제의 전단결합강도에 관한 연구

  • Yu, Hwa-Sung (Department of Conservative Dentistry, Division of Dentistry, Graduate School, KyungHee University) ;
  • Choi, Gi-Woon (Department of Conservative Dentistry, Division of Dentistry, Graduate School, KyungHee University) ;
  • Choi, Kyung-Kyu (Department of Conservative Dentistry, Division of Dentistry, Graduate School, KyungHee University) ;
  • Park, Sang-Jin (Department of Conservative Dentistry, Division of Dentistry, Graduate School, KyungHee University)
  • 유화성 (경희대학교 치과대학 치과보존학교실) ;
  • 최기운 (경희대학교 치과대학 치과보존학교실) ;
  • 최경규 (경희대학교 치과대학 치과보존학교실) ;
  • 박상진 (경희대학교 치과대학 치과보존학교실)
  • Published : 2000.12.05

Abstract

In this study, shear bond strength of two bonding systems were measured and appearance of dentin surfaces were observed with SEM according to the storage time of eugenol on dentin surface, thus evaluated the effect of eugenol on bond strength of two dentin bonding systems. Control groups were directly bonded to dentin surface with One Step, Prime & Bond 2.1. Experimental groups were divided into experimental I and II according to dentin bonding agents. After eugenol application, dentin surfaces were bonded with One Step and Prime & Bond 2.1 according to the each storage time of immediately, 3min, 24hour, 48hour and 1week, and then control and experimental groups were filled with light cured composite resin(Z-100). After 24 hours water storage at $37^{\circ}C$, all samples were subjected to a shear load to fracture at a cross head 1.0mm/min with Instron universal testing machine(No. 4467). Etched dentin surface storaged for each time of immediately, 3min, 24hour, 48hour and 1 week after eugenol application were observed under Scanning Electron Microscope(Hitachi S-2300) at 20kvp. The data were evaluated statistically with two-way ANOVA and Tukey's HSD. The results were as follows; 1. Shear bond strengths were higher in control groups than in the experimental groups. 2. As storage time was increased after eugenol application, the shear bond strengths were decreased in experimental groups. 3. In experimental I, II the shear bond strengths were the lowest in which storage time was 1 week after eugenol application. 4. As storage time was increased after eugenol application, etched dentin surfaces showed obstructed dentinal tubule.