A Study on the Adhesiveness between Polyurethane Sheet for Maxillofacial Prostheses and Autopolymerizing Acrylic Resin in Various Polymerization Methods

다양한 중합방법에 따른 악안면 보철용 폴리우레탄과 자가중합 레진 간의 결합력에 관한 연구

  • Kim, Doo-Yeol (Department of Prosthodontics Graduate School Dankook University) ;
  • Cho, In-Ho (Department of Prosthodontics Graduate School Dankook University)
  • 김두열 (단국대학교 치과대학 치과보철학교실) ;
  • 조인호 (단국대학교 치과대학 치과보철학교실)
  • Published : 2000.06.30

Abstract

The field of maxillofacial prosthetics is concerned with the prosthetic reconstruction of missing head and neck tissue. Currently, facial prostheses are usually applied in cases of defects caused by the surgical removal of tumors or congenital defects. While silicone has been most widely used for the reconstruction of missing maxillofacial defects, it does not have ideal physical properties. Therefore, bonding a thin polyurethane sheet to silicone prostheses was recommended. In this case skin adhesives were used for the retention of maxillofacial prostheses. But retention of devices has always been problematic. The contributions of implants can be made to solve these problems. Implants have reduced the need for adhesive use, simplifying cleaning procedures and thus extending the life of the prostheses. For implant-retained prostheses, retentive matrix is necessary to hold attachments and/or magnets. The retentive matrix is usually fabricated with autopolymerizing acrylic resin or visible light- polymerized resin. The purpose of this study was to compare the adhesion-in-peel force of silicone adhesive to autopolymerizing acrylic resin and polyurethane sheet with two different surface textures : pumice polish only or retention groove, and three surface primers : Dow corning 1205 primer or Dow corning S-2260 primer or FactorII A-304 primer, and two polymerization methods : room temperature or dry heat oven. The t-peel bond strength of specimens was determined as described in ASTM Standard D1876-72. The results were statistically analyzed using the ANOVA test, multiple range test and t-test The results were as follows. 1. The t-peel bond strength of A-304 primer was the highest and statistically higher than that of S-2260(p<0.05). 2. The t-peel bond strength of specimens with retention groove was statistically higher than that of specimens polished with pumice(p<0.05). 3. The t-peel bond strength of specimens polymerized in dry heat oven was statistically higher than that of specimens in room temperature(p<0.01).

Keywords