연속 정련축소 장치의 특성 연구 -로터드럼형과 컨베이어형-

A Study on the Characteristics of Continuous Scouring and Shrinking Equipment -Rota-drum and conveyor type-

  • 허만우 (경일대학교 공과대학 섬유패션공학과) ;
  • 서말용 (한국섬유개발연구원)
  • 발행 : 2000.02.01

초록

In this study, polyester DTY faille(yoryu) and N/NP microfiber fabrics were pretreated (desizing, scouring and shrinking) by Continuous Scouring and Shringking Equipment with rota-drum and conveyor type in which types were different with retaining method. The results were as follows. The shrinkage ratio of wp/wf direction of DTY fabrics scoured by conveyor type was 1.5/23% higher than those by rota-drum type at $97^\circ{C}$ with 10min. treatment. In this case, The shrinkage ratio of wp/wf direction by those types was about 15/27%, respectively. The shrinkage ratio of wp/wf direction of N/NP microfiber fabrics scoured by conveyor type was 1.5/23% higher than that by rota-drum type at $97^\circ{C}$ with 10min. treatment. The size add-on of DTY fabrics scoured at $97^\circ{C}$ with 10min. treatment by conveyor type and by rota-drum type were 0.15% and 0.42%, respectively. The size add-on of DTY fabric treated by rota-drum type decreased until 9min. of treated time, but increased after 9min. The size add-on of N/NP microfiber fabrics treated by conveyor type was decreased by increasing temperature and treated time, while the size add-on of that treated by rota-drum type was decreased until 6min. treated time and increased after 6min. The size add-on of N/NP microfiber fabrics treated by conveyor type at $97^\circ{C}$ for 10min. was 0.3% lower than that by rota-drum type.

키워드