Abstract
In order to study the effect of high energy ball milling on the $Mg_2Ni+Ni$, $Mg_2Ni+0.5Ni+0.5Al$ powders, we have investigated on the discharge properties, microstructures. The powder size of samples decreased as ball milling time. From the XRD results, the crystal structure of $Mg_2Ni+Ni$ mixed powders were changed to amorphous or nano-structure after 60hr ball milling. The discharge capacities of both $Mg_2Ni+Ni$ and $Mg_2Ni+0.5Ni+0.5Al$ powders increased, with increasing ballmilling time, the maximum capacity(342mAh/g) was shown for the 60 hrs ballmilled $Mg_2Ni+Ni$ sample. The capacity decreased drastically after a few charge-discharge cycles.