Dependence of the lithium ionic conductivity on the B-siteion substitution in $(Li_{0.5}La_{0.5})Ti_{1-x}M_xO_3$

  • Kim, Jin-Gyun (Department ofMaterials Science and Engineering. Korea Advanced Institute of Science and Technology) ;
  • Kim, Ho-Gi (Department ofMaterials Science and Engineering. Korea Advanced Institute of Science and Technology)
  • Published : 1998.11.01

Abstract

The dependence of the ionic conductivity on the B-site ion substitution in (Li0.5La0.5)Ti1-xMxO3 (M=Sn, Zr, Mn, Ge) system has been studied. Same valence state and various electronic configuration and ionic radius of Sn4+, Zr4+, Mn4+ and Ge4+(4d10(0.69$\AA$), 4p6(0.72$\AA$), 3d10(0.54$\AA$) and 3d3(0.54$\AA$), respectively) induced the various crystallographic variaton with substitutions. So it was possibleto investigate the crystallographic factor which influence the ionic conduction by observing the dependence of the conductivity on the crystallographic factor which influence the ionic conduction by observing the dependence of the conductivity on the crystallographic variations. We found that the conductivity increased with decreasing the radii of B-site ions or vice versa and octahedron distortion disturb the ion conduction. The reason for this reciprocal proportion of conductivity on the radius of B-site ions has been examined on the base of the interatomic bond strength change due to the cation substitutions. The results were good in agreement with the experimental results. Therefore it could be concluded that the interatomic bond strength change due to the cation substitutions may be the one of major factors influencing the lithium ion conductivity in perovskite(Li0.5La0.5) TiO3system.

Keywords