A STUDY ON THE FRACTURE STRENGTH OF THE IPS-EMPRESS CERAMIC CROWN ACCORDING TO MARGIN TYPE

IPS-Empress 도재관의 변연형태에 따른 파절강도에 관한 연구

  • Kim, Hyun-Soo (Department of Prosthodontics, College of Dentistry, Wonkwang University) ;
  • Ju, Tae-Hun (Department of Prosthodontics, College of Dentistry, Wonkwang University) ;
  • Oh, Sang-Chun (Department of Prosthodontics, College of Dentistry, Wonkwang University) ;
  • Dong, Jin-Keun (Department of Prosthodontics, College of Dentistry, Wonkwang University)
  • 김현수 (원광대학교 치과대학 보철학 교실) ;
  • 주태훈 (원광대학교 치과대학 보철학 교실) ;
  • 오상천 (원광대학교 치과대학 보철학 교실) ;
  • 동진근 (원광대학교 치과대학 보철학 교실)
  • Published : 1997.07.01

Abstract

The purpose of this study was to compare the fracture strength of the IPS-Empress ceramic crown according to margin types such as bevel, shoulder, rounded shoulder, shoulder with bevel, rounded shoulder with bevel and bevel with groove. After 10 metal dies were constructed for each group, the IPS-Empress ceramic crown were fabricated and each crown was cemented on each metal die with Bistite resin cement. The cemented crowns mounted in the testing jig were inclined 30 degree and universal testing machine (Zwick 1456 41, Zwick Co., Germany) was used to measure the fracture strength. The obtained results were as follows : 1. The fracture strength of the crown with rounded shoulder was the highest of all. The mean fracture strength was 484N in rounded shoulder, 357N in bevel, 341N in rounded shoulder with bevl, 300N in shoulder with bevel, 280N in shoulder and 275N in bevel with groove. 2. The fracture strength of rounded shoulder was statistically different from those of shoulder with bevel, shoulder and beve41 with groove. 3. In the strain at fracture, there was no significant difference among each group. 4. The fracture mode of the crown was similar and most of fracture line began at the loading area and extended through proximal surface perpendicularly to the margin, irrespective of margin type.