Abstract
The reactions between an active metal brazing alloy and interlayers together with the effects of interlayer type on the interfacial microstructure change were investiaged for silicon nitride/stainless steel joint. The bending strengths were measured for joints with Mo, Cu, Ni interlayer type of different thicknesses. It was found that the interlayer with a low yield strength value is effective to improve the bending strength of the Si3N4/stainless steel joint. The maximum joint strength obtained at room temperature for a laminated Cu/Mo interlayer was about 460 MPa. The combined use of Mo and thin Cu layer was found to be effective in enhancing the bending strength for the Si3N4/S.S.316 joint.