The Study on the Weight loss Finishing for the mixture Silk/Polyester II. The Weight loss Finishing for the Spun silk/Polyester

Silk/Polyester 혼섬유 재료의 감량가공에 관한 연구 II. Spun silk/Polyester 혼섬유의 감량가공

  • Published : 1994.06.01

Abstract

The weight loss for the mixture (spun silk/PET) was tested to investigate the effects of weight loss accelerator on the degumming and weight loss. The degumming loss of spun silk was decreased while the wigth loss of polyester(PET) was increased depending on the increased of weight loss accelerator concentration. The proper degumming of spun silk was obtained and simultaneously the weight loss of PET was high for the spun silk/PET "A" and "B" type. The proper degumming of spun silk was obtained but the weight of PET was loss for the spun silk/PET "D" and "E" type. The degumming curve in spun silk part was showed the typical degumming curve but the weight loss of PET was increased depending on the increased of treatment time in the weight loss for the fabric composed of spun silk/PET.or the fabric composed of spun silk/PET.

견방사와 PET로 구성된 혼섬유 재료에 대해 여러가지 조건에서 알칼리 감량을 실시하여 감량율을 조사하고, 감량촉진제가 정련, 감량에 미치는 영향에 대해 검토한 결과를 요약하면 다음과 같다. 1) 감량촉진제와 농도 증가에 따라 견방사의 감량은 감소하여 강알칼리욕에서도 적당한 정도의 감량율을 얻을 수 있었다. 2) PET "A", "B"와 견방사로 된 혼섬유의 감량에서 견방사는 피브로인의 손상이 없는 정도의 적당한 감량이 얻어졌고, PET의 감량도 동시에 이루어 질 수 있었다. 3) PET "D", "E"와 견방사로 된 혼섬유의 감량에서, 견방사는 적당한 감량이 이루어 질 수 있었으나 PET의 감량율은 미미하였다. 4) 견방사와 PET로 된 교직물의 감량에 있어서, 견방사 분분은 전형적인 연감곡선 형태를 나타내 감량평형을 보였으나 PET는 처리시간의 경과에 따라 감량율이 계속해서 증가하였다. 보였으나 PET는 처리시간의 경과에 따라 감량율이 계속해서 증가하였다.

Keywords