Annealing Effect on the Microwave Dielectric Properties of the BaO-SmS12TOS13T-TiOS12T Ceramics

BaO-Sm2O3-TiO2 세라믹스의 마이크로파 유전특성에 미치는 어닐링 효과

  • Published : 1994.05.01

Abstract

In this study, the structural and microwave dilelectric properties of 0.15BaO-0.15SmS12TOSI3T-0.7TiOS12T ceramics with sintering and annealing conditions were investigated. In the specimen sintered at 1350 [$^{\circ}C$], dielectric constant and quality factor were good values of 80.19,2006 (fS10T=4.6851[GHz]). To improve the $\tau$S1fT of specimen which was manufactured by the optimumsintering condition (1350[$^{\circ}C$],2[Hr.]), annealed from 2[hr.] to 16[hr.] at the annealing temperature of 1200 [$^{\circ}C$]. Increasing the annealing time, dielectric constant was almost constant and quality factor was increased. In the specimen of 4[hr.] annealed, the temperature coefficient of resonant frequency was minimum value, and increased with increasing the annealing time.

Keywords