Abstract
Spinel powders were synthesized at the comparatively low-temperature range(800~90$0^{\circ}C$) by the emulsion-hot kerosene drying method and the effects of kerosene-evaporative conditions on powder characteristics were investigated. In emulsion drying, more unagglomerated and sinterable powders could be synthesized through rapid evaporation of emulsion at the higher kerosene temperature. The completion of formation reaction of spinel observed at the low-temperature range confirmed the high reactivity of powders. The relative theoretical density and the fracture toughness of spinel pellets sintered at 1$650^{\circ}C$ for 4hrs. were 98% and 2.1MN/m3/2, respectively.