Abstract
Pb(Zr0.52Ti0.48)O3 powders were prepared by hydrothermal synthesis. Using soluble salts such as Pb(NO3)2, TiCl4 and ZrOCl2$.$8H2O and oxide such as PbO and TiO2 as starting materials, PZT powder was hydrothermally synthesized at the temperature range between 150$^{\circ}C$ and 200$^{\circ}C$. The result showed that reactivity by alkali was decreased in the sequence of Pb(NO3)2, TiCl4, ZrOCl2, PbO, TiO2 and ZrO2. Using the first three soluble salts, PZT powder was synthesiged at 150$^{\circ}C$ for 1hr. In PbO-TiCl4-ZrOCl2 system, PZT powder was synthesized at 150$^{\circ}C$ for 8rs. In Pb(NO3)2-TiO2-ZrOCl2 system, PZT powder was synthesized at 150$^{\circ}C$ for 16hrs, in PbO-TiO2-ZrOCl2 system, the powder was synthesized at 200$^{\circ}C$ for 8hrs.