Abstract
Korean red pine (Pinus densiflora S. et. Z.) and pitch pine(Pinus rigida Mill) $5{\times}10cm$ dimension lumber were dried in a kiln providing a cross-circulation velocity of 5 m/sec at dry-and wet-bulb temperatures of 116 and $71^{\circ}C$, followed by 3 hours at 91 and $85^{\circ}C$. Compared to dimension lumber dried lumber were as follows. 1. To dry to 10 percent moisture content, the high-temperatures schedule of Korean red pine and pitch pine lumber took less than one seventh the time required by the conventional kiln drying schedule. 2. High-temperature drying rate and conventional drying rate to 10 percent moisture content of Korean red pine lumber were 2.75 and 0.35%/hr, and those of pitch pine lumber were 3.38 and 0.46%/hr respectively. 3. Compared to lumber of both species on conventional schedule, moisture gradient of high-temperature lumber was greater. 4. Compared to lumber on conventional schedule, maximum surface checking of high-temperature lumber of both species was severer, and maximum end checking of high-temperature lumber of both species was similar to that of lumber on conventional schedule. 5. Compard to lumber on conventional schedule, Korean red pine lumber dried at high temperature showed more honeycombing, but pitch pine lumber dried at high-temperature showed significantly slighter honeycombing. 6. Compared to lumber on conventional schedule, the high-temperature lumber showed less warping lumber of both species. 7. Collapse and casehardening of Korean red pine and pitch pine lumber on both scheules were slight.