소환온도(燒還溫度)와 재(再) 주조금속(鑄造金屬) 함량비(含量比)가 Ni-Cr계(係) 비귀금속(非貴金屬) 합금(合金)의 가주성(可鑄性)에 미치는 영향

The Influence on Castability of Nickel-Chromium Alloys according to Burn-out Temperature and Recast Content Ratio

  • 이효병 (광주보건전문대학 치기공과)
  • Lee, Hyo-Byeang (Dept. of Dental Lab. Technology Kwangju Health Junior College)
  • 발행 : 1986.06.01

초록

The castability of base metal alloys for dental casting in influenced by burn-out temperature and recent percentage. Burn-out temperatures for casting are set at 200$^{\circ}F$ interval from 1000$^{\circ}F$ to 1800$^{\circ}F$. According to recast metal percent in new cast alloy metal alloys are tested. The results are as followings: 1. In the new alloy(100%), the castability is the most. 2. The burn-out temperature in 1600$\sim$1800$^{\circ}F$, castability of 100% new alloy was more four times than of 50% new alloy plus 50% recast alloy. The using of 50% new alloy and 50% recast alloy, therefore, was unlike in castability. 3. The burn-out temperature in 1600$^{\circ}F$, castability of 100% new alloy was more than four times in soaking 20 minutes, but there was no any difference at 18700$^{\circ}F$. 4. It is investigated that the optimal burn-out temperature is 1600$^{\circ}F$ for the C & B alloy.

키워드