수종치과매몰재(數種齒科埋沒材)의 열팽창계수(熱膨脹係數)에 관(關)한 실험적(實驗的) 연구(硏究)

AN EXPERIMENTAL STUDY ON COEFFICIENT OF THERMAL EXPANSION OF DENTAL INVESTMENTS

  • 이명종 (서울대학교 치과대학 보존학교실)
  • Lee, Myung-Jong (Dept. of Operative Dentistry, College of Dentistry, Seoul National University)
  • 발행 : 1979.12.31

초록

The purpose of this study was to measure thermal expansions of dental investments, Biovest(Casting Investment. Dentsply International INC, U.S.A.), Multi-Best (Use for all dental chrome-cobalt alloys, The Ransom & Randolph Co. U.S.A.), Kerr(Inlay Investment. Sybron Kerr, U.S.A.), O. K. (Inlay Investment. Shofu Dental MFG, Co. Japan), Whip-Mix (Cristobalite Inlay Investment. Whip-Mix Corporation. U.S.A.). Thermal expansion of specimens(5mm in diameter and 50mm in length) was measured by a dilatometer at the temperature range from $20^{\circ}C$ to $700^{\circ}C$ by comparing expansion between standardized quartz and experimental specimens with heating rate about $300^{\circ}C$/hr. The following results were obtained. 1. The coefficient of thermal expansion of Biovest was $15{\times}10^{-6}/^{\circ}C$ in the water powder ratio 18/100 and $14{\times}10^{-6}/^{\circ}C$ in the water powder ratio 28/100. Those of Multi-Best were $9{\times}10^{-6}/^{\circ}C$ in the water powder ratio 14/100 and $7{\times}10^{-6}/^{\circ}C$ in the water powder ratio 24/100. 2. The coefficient of thermal expansion of Kerr were $17{\times}10^{-6}/^{\circ}C$ in the water powder ratio 38/100 and $14{\times}10^{-6}/^{\circ}c$ in the water powder ratio 48/100. Those of O. K. were $9{\times}10^{-6}/^{\circ}C$ in the water powder ratio 33/100 and $7{\times}10^{-6}/^{\circ}C$ in the water powder ratio 43/100 3. The coefficient of thermal expansion of Whip-Mix were $14{\times}10^{-6}/^{\circ}C$ in the water powder ritio 40/100 and $12{\times}10^{-6}/^{\circ}c$ Fein the water powder ratio 50/100. Those of Hi-Heat were $11{\times}10^{-6}/^{\circ}c$ in the water powder ratio 28/100 and $10{\times}10^{-6}/^{\circ}c$ in the water powder ratio 38/100.

키워드