Fundamental Research on Compressive Strength Recovery of Excessive High-volume Fly Ash Mortar

Fly Ash가 다량치환된 모르타르의 압축강도 회복에 관한 기초적 연구

  • Published : 2019.05.15

Abstract

The purpose of the research is assessing the possibility of strength recovery for mortar added with accidently high amount of fly ash. For compressive strength at 28 day, the sample painted with sodium hydroxide showed higher compressive strength than the sample painted with calcium hydroxide. Regarding the curing conditions, the curing temperature 65℃ provided better conditions than the curing temperature 20℃ in aspect of solution penetration depth and reactivity of fly ash. In the case of drying after saturation, the case painted with sodium hydroxid 65℃ showed the clearest engrossing mark.