Designed compressive strength assurance method within 28 days of management period for winter period concrete contain various SCMs
한중콘크리트의 관리재령 연장을 이용한 설계기준강도 확보 기법
Abstract
The purpose of the research is suggesting the temperature compensation strength for Unicode of constructure standard from Ministry of land, infrastructure and transport. As a result, for the concrete mixture with 100 % OPC, 6, and 3 MPa of compensating strength values were necessary when the temperature were from 4 to 9℃, and from 9 to 17℃, respectively. Additionally, when the temperature was higher than 17℃, compensating strength value was not necessary. In the case of 20 % of blast furnace slag replaced concrete mixture, 9, 6, and 3 MPa of compensating strength values were necessary when the temperature were from 4 to 6℃, from 6 to 12℃, and higher than 17℃, respectively.