산화마그네슘을 활용한 경화체의 지연제 첨가율에 따른 접착강도 특성

Adhesion Strength Properties of Matrix Using Magnesia Accroding to Potassium Phosphate Addition Ratio

  • 김태현 (한밭대학교 건설환경조형대학, 건축공학과) ;
  • 신진현 (한밭대학교 건설환경조형대학, 건축공학과) ;
  • 이상수 (한밭대학교 건설환경조형대학, 건축공학과)
  • 발행 : 2016.05.19

초록

Most of the construction adhesive may contain harmful component to the human body with an organic adhesive. In addition, when the adhesive caused hydroquinone, alkyl benzophenone, etc, also it raises the skin diseases to workers. Therefore, the inorganic adhesive development is necessary. This study was a study to know adhesive strength properties that adhesive using a magnesium oxide according to the addition ratio of the retarder. It has experiments to two types of magnesium oxide and type and ratio of retarder differently.