Temperature History of the Slab Concrete applying Revised Bubble Sheet with Heating Cable

열선 매입과 열선 및 버블시트 조합의 개량형 버블시트를 포설한 슬래브 콘크리트의 온도이력 특성

  • Published : 2013.11.15

Abstract

In this study, the results are compared with the case of the concrete with embedded heating wire to verify the performance of the IB made in order to improve the workability and affordability, and to determine the effectiveness of early frost damage prevention. The IB was made using the 5W heating wire and layed on the upper surface of the concrete. The temperature was reduced to below 0℃ approximately within 24 hours, then approached the external temperature thereafter. On the other hand, when the 20W heating wire was used to make the IB and applied the same way, the temperature remained around -2 to 3℃ on the average even through the temperature was reduced to below 0℃, due to the heating wire with relatively large heating capacity. It appeared to reach 85% of the direct heating by embedding the heating wire relatively deeper in the concrete. However, it was determined that using the IB made with the 20W heating wire will prevent the early frost damage to some degree in -10℃.

Keywords