분말 압출 공정에서 온도 유지시간 제어를 통한 미세기어의 내피로성 향상 연구

Improvement of fatigue resistance of the miniature gear by controlling holding time of temperature in the hot powder extrusion process

  • 김진우 (부산대학교 하이브리드소재솔루션 협동과정) ;
  • 이경훈 (부산대학교 정밀기계공학과) ;
  • 황대원 (부산대학교 정밀기계공학과) ;
  • 김병민 (부산대 기계공학부)
  • 발행 : 2009.10.08

초록

This paper was designed to fabricate the miniature spur gear with pitch circle of 1.8 by hot extrusion process of mechanically alloyed Zn-22wt%Al powder at various temperature. The mechanical alloying was preformed for ball milled times of 8h, 16h and 32h by the planetary ball milling. Mechanically alloyed powders were compacted cylindrical performs. Extrusions of the miniature spur gear using the alloyed powder were carried out at different extrusion temperatures. The extruded spur gear was sintered for 2h at $350^{\circ}C$ in argon atmosphere. The friction between the die and the powdered billet and the internally different density due to complex product shape cause the internal crack. To overcome the mentioned problems, high dimensional accuracy at cross section of the spur gear and uniform Vickers hardness could be obtained by graphite lubricant and controlling holding time.

키워드