The Exploration on Early Age Deformation of HPC by FBG Strain Sensor

  • Published : 2008.04.24

Abstract

For high performance concrete, due to its low water cement ratio (water binder ratio) and addition of mineral admixtures, pretty high autogenous shrinkage and thermal deformation occur at very early age of casting (especially before hardening). This may lead to early age cracking of HPC structures, and then may influence the durability of HPC. This paper has monitored the early age properties of HPC successfully by embedded FBG strain sensor. The results showed that the deformation increased rapidly within the first day after HPC casting. And its value is up to $85{\mu}{\varepsilon}$, which is the 30% of two-month deformation ($280{\mu}{\varepsilon}$). Considering the durability and permeability of HPC, the first-day deformation is pretty high and can not be neglected. Also the superior capability of FBG sensors such as continuity, stability and multiplexed technique etc, has been demonstrated.

고강도 콘크리트는 낮은 물-시멘트 비와 혼화제의 첨가로 인해 타설 후 극 초기재령에서 큰 자기수축과 온도변형이 발생한다. 이것은 고강도 콘크리트 구조물의 초기재령에서의 균열을 초래할것이고, 고강도 콘크리트의 내구성에 영향을 미칠 것 이다. 그러므로 고강도 콘크리트의 초기재령 특성에 집중할 필요가 있다. 이 논문에서는 매설형 FBG 센서를 이용하여 고강도 콘크리트의 초기재령 특성을 모니터링 하였다. 결과에서는 고강도 콘크리트 타설 후 하루동안 변형이 급격히 증가함을 보여 주었다. 그리고 변형량의 값은 $85{\mu}{\varepsilon}$ 이상이며, 두달간의 변형량($280{\mu}{\varepsilon}$)의 30%에 해당한다. 고강도콘크리트의 내구성과 침투성을 고려하면, 첫째날의 변형률은 꽤 높아 무시할 수 없는 수치이다. 또한 연속성, 안정성, 다양한 복합기술 등 FBG 센서의 보다 높은 성능이 증명 되었다.

Keywords