There are two ways to reduce cement content for a given quality level(strength, workability etc.) in concrete. First, reducing the required paste volume by varying the shape or the grading of aggregates. Secondly, holding the paste volume constant while replacing cement volume with mineral admixtures or mineral fillers. And It will also be proved that the required minimum paste volume is independent of the paste composition, provided the paste composition is in a reasonable range. In this study, therefore, we have an object to determine the required minimum paste volume for a given workability level. For this purpose, we tried the following experiments: vary the paste volume for the three different grading of aggregates and determine the minimum paste volume to achieve a certain level of workability with high-range water reducing admixture.

일정 수준의 콘크리트 품질 수준을 유지하면서 시멘트 사용량을 줄이는 방법으로는 첫째, 다양한 입형과 입도의 골재 사용, 둘째, 사용되는 시멘트의 일부를 광물질 혼화재 및 광물질 채움재로 대체하는 방법등이 있다. 또한 페이스트의 구성성분이 합리적인 범위라면, 일정 수준의 품질을 유지하기 위하여 필요한 최소 페이스트 체적은 페이스트 구성성분과는 무관할 것으로 생각된다. 따라서 본 연구에서는 일정 수준의 워커빌리티를 유지하기 위하여 콘크리트에서 필요로 하는 최소 페이스트 체적을 결정하고자 하였다. 이를 위하여 입도가 다른 3종류의 골재에 대하여 페이스트의 체적을 변화시키면서, 고성능감수제를 사용하여 모르타르의 플로우값 130을 유지하는데 필요한 최소 페이스트체적에 대하여 연구하였다.

Keywords