Friciton stir welding of type 304 stainless steel

304 스테인레스 스틸의 마찰교반접합

  • 이창용 (성균관대학교 신소재공학부) ;
  • 최돈현 (성균관대학교 신소재공학부) ;
  • 표성은 (성균관대학교 신소재공학부) ;
  • 이원배 ((주)포스코 기술 연구소) ;
  • 이종봉 ((주)포스코 기술 연구소) ;
  • 연윤모 (수원과학대학 신소재응용과) ;
  • 정승부 (성균관대학교 신소재공학부)
  • Published : 2007.11.15

Abstract

The butt and lap configurational friction stir welding of type 304 stainless steel was conducted in this study. The sound joints were obtained by WC tool. As the welding distance increased, tool deformation gradually increased at the pin edge. The discoloration by oxidation was observed at the top surface of the joint, a sufficient heat-input was required to avoid the welding defect owing to the lack of stirring at the welding start point. Very fine grains were observed in the stir zone, and the grain coarsening was not observed in the heat affected zone.