Abstract
This paper was accomplished for analyzing the reason of the above deterioration happened on the deck of concrete bridge. The bridge was constructed at 660m above the sea level having more freezing and snowing days. Therefore, it is placed on the particular condition sprinkling $CaCl_2$ enough for keeping up with moderate traffic condition. When it is considered to the former condition, the bridge can be assumed to potentialities for combined deterioration with freezing-thawing under sprinkling deicing chemical. Core specimens were gathered from the concrete deck for clearing the reason of the above deterioration exactly, and it is used for various tests for measuring the compressive strength, elastic modulus, content of $Cl^-$, freezing-thawing at the fresh and salt water. As a result of freezing-thawing test, the specimen at the fresh water has over 90$\%$ of durability factor, but another specimen at 1$\%$ of salt water has 0$\%$ of durability factor at 140 cycles of the freezing-thawing. The result means that frost damage is sccelerated at the salt water. Therefore, the deterioration of the concrete deck is estimated to be occured by combined effects of freezing-thawing and chloride ion attack.