Changes in Microstructures of AA3103 sheets deformed by ECAR

ECAR 가공한 AA3103 판재의 미세조직 변화

  • Published : 2004.05.01

Abstract

Samples of the aluminum alloy 3103 sheets were repeatedly deformed by ECAR up to twelve passes. Shear textures developed after the first passage of ECAR. However, the intensity of shear texture components decreased with increasing number of ECAR passages. Observations by TEM and EBSD revealed that the degree of misorientations within the deformed grains increased with increasing number of ECAR passes. Changes in textures and microstructures were hardly observed during recrystallization anneal. Upon subsequent annealing, the samples deformed by a large number of ECAR passes displayed a continuous grain growth. A higher deformation by ECAR resulted in a slower softening, which reflects the stability of ultra-fine grains against the grain growth.