Abstract
The lead zirconate titanate, $Pb(Zr_{0:52}Ti_{0:48})O_3$, films of $0.5\;{\mu}m,\;1\;{\mu}m$ and $2\;{\mu}m$ thickness were fabricated on $Pt/Ti/SiO_2/Si$ substrate by the rf magnetron sputtering method. The PZT films were annealed using by a rapid thermal annealing (RTA) method. The thickness dependence of the film structure, dielectric properties, Polarization-electric field hysteresis loops and capacitance-voltage characteristics were investigated over the thickness range of $0.5\;{\mu}m,\;1\;{\mu}m$ and $2\;{\mu}m$. According to the XRD patterns of the films, (110) peak intensity increases with film thickness increased. The increase of PZT films thickness leads to the decrease of the remanent polarization and the dielectric constant.